TRAPPING OF HYDROGEN BY PRECIPITATE TiC IN LOW CARBON STEEL
by XIAN Aiping; LI Peiji; WANG Yikang; LI Xun(H. Lee) (Institute of Metal Research; Academia Sinica; Shenyang)
Cite this article: 

by XIAN Aiping; LI Peiji; WANG Yikang; LI Xun(H. Lee) (Institute of Metal Research; Academia Sinica; Shenyang). TRAPPING OF HYDROGEN BY PRECIPITATE TiC IN LOW CARBON STEEL. Acta Metall Sin, 1986, 22(3): 1-8.

Download:  PDF(1399KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influence of Ti on hydrogen diffusion in low carbon steel was studied by Davanathan's electrochemical method. The experimental results show that the strong trapping of hydrogen is appeared in the steel in which the Ti precipitated as dispersed TiC during aging after solution treatment. The trapping energies of the precipitation of dispered TiC are evaluated as 27.88±0.18 and about 21 kJ/mol respectively before and after the α→γ phase transformation of the steel. However, these do not coincide with the value of 94.55 kJ/mol reported by Pressouyre. The lowest apparent diffusion coefficient of hydrogen in the steel Fe-0.2Ti-0.1C is found after solution-treated at 1200℃ and aged at 550℃. It seems to be caused by the low temperature precipitate TiC with non-cubic structure and by many lattice vacancies which distort the local periodical potential fields around it.
Received:  18 March 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I3/1

1 Oriani, R.A., Acta Metall., 18 (1970) , 147.
2 Pressouyre, G.M., Metall. Trans., 10A (1979) , 1571.
3 Kim, K.B.; Pym, S.I., Arch. Eisenhuettenwes., 53 (1982) , 397.
4 Choo, W.Y.; Lee, J.Y., J. Mater. Sci., 17 (1982) , 1930.
5 山川宏二;鹤田孝雄;吉沢四郎,防食技术,30 (1981) ,443.
6 王明中;田中卓;肖纪美等,北京钢铁学院学报,(1985) .№1,47.
7 Pressouyre, G.M.; Bernstein, I.M., Metall. Trans., 9A (1978) , 1571.
8 坂本芳一,热处理,23 (1983) ,26.
9 Takahshi, I.; Matsumoto, Y.; Aruga, I., KAWASAKI Steel Technical Report №3, 1981, p. 57.
10 冼爱平,中国科学院金属研究所硕士论文,(1985) .
11 Devanathan, M.A.V.; Stachurski, Z., Proc. R. Soc., A270 (1962) , 90.
12 Kiuchi, K.; Mclellan, R.B., Acta Metall., 31 (1983) , 961.
13 Meyer, L.; Buehler, H.E.; Heister, kamp, F.; Jackel G.; Ryder, P.L., Arch. Eisenhuettenwes., 43 (1972) , 823.
14 Lee, H.G.; Lee, J.Y., Acta Metall., 32 (1984) , 131.
15 Fast. J., 金属中的气体,刁伟涛等译,冶金工业出版社,1983.
16 Shirley, A.I.; Hall, C.K., Acta Metall., 32 (1984) , 49.
17 方俊鑫;陆栋;固体物理学,下册,上海科学技术出版社,(1981) ,p.61.
18 Aono, M.; Hou, Y.; Souda, R.; Oshima, C.; Otani, S.; Ishizawa, Y., Phys. Rev. Lett., 50 (1983) , 1293.
19 Mcnabb, A.; Foster, P.K. Trans. Metall. Soc. AIME, 227 (1963) , 618.
20 Quick, N.R.; Johnson, H.H., Acta Metall., 26 (1978) , 903.
No related articles found!