Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (2): 119-156    DOI:
Current Issue | Archive | Adv Search |
ON THE CRYSTALLIZATION OF AMORPHOUS Ni-BASE ALLOY
WANG Yuming; MENG Zhaofu; WANG Zhao (Jilin University; Changchun)
Cite this article: 

WANG Yuming; MENG Zhaofu; WANG Zhao (Jilin University; Changchun). ON THE CRYSTALLIZATION OF AMORPHOUS Ni-BASE ALLOY. Acta Metall Sin, 1986, 22(2): 119-156.

Download:  PDF(1593KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The crystallization of amorphous Ni_(83)Cr_7Fe_3Si_4B_3 alloy was investigated under dynamic heating and isothermal annealing conditions. An identical crystallization and unaltered phases are revealed under both treatments. However, the initial crystallization is mainly due to the nucleation of crystals under dynamic heating, while the crystal growth plays a major role under isothermal annealing. It has also been measured that the microhardness approached its highest value just before the specimen being totally crystallized.
Received:  18 February 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I2/119

1 Tiwari, R.S.; Ranganathan, S.; Heimendahl, M.V., Z. Metall, 72 (1981) , 563.
2 Scott, M.G., J. Mater. Sci., 13 (1978) , 291.
3 Von Heimendahl, M.; Maussner, G., J. Mater. Sci., 14 (1979) , 1238.
4 Chang, H.; Sastri, S., Metall. Trans., 8 (1977) , 1063.
5 Waseda, Y; Okazaki, H.; Masumoto, T.J. Mater. Sci., 12 (1977) , 1927.
No related articles found!