STRUCTURAL FEATURE OF CAST Al-BASE COMPOSITE
JI Shichen; LI Ying'ao; WANG Guozhi (Institute of Metal Research; Academia Sinica; Shenyang)
Cite this article: 

JI Shichen; LI Ying'ao; WANG Guozhi (Institute of Metal Research; Academia Sinica; Shenyang). STRUCTURAL FEATURE OF CAST Al-BASE COMPOSITE. Acta Metall Sin, 1986, 22(1): 64-145.

Download:  PDF(2456KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An observation was carried out on the feature of microstructure, fracture and worn surface of the Al-base composite prepared by rheocasting with graphite, SiC and SiO_2. The a solid solution, Si, CuAl_2 and allied eutectics are found to nucleate and to grow up along the surface of particulates added during solidification of the compslurry. The short-range movement of the particulates may distribute more uniformly in matrix owing to rapidly raising temperature of the composlurry before casting. Over the particulate, a transition layer connects with the matrix, and the active element Mg accumulates more or less. Thus, the firm bond is joined between the particulate and matrix, and it makes no more pore and crack on the microstructure of fractured or worn surface.
Received:  18 January 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I1/64

1 Mehrabian, R.: Backman, D.G.: Murty, Y,Y.: ttong, S.: Levi, C.. 9th SDCE (Society of Die Casting Engineers) Int. Die Casting Exposition and Congress Paper, No. G. T. 77 083. June 6-9,1977, Mikuaukee, Wisconin.
2 Gibson. P. R.; Clegg, A.J.: Das, A.A.. Foundary Trade J., 155 (1982) , № 3232, 253-256, 262-267.
3 #12
4 Sato, A.: Mehrabian, R.. Metall. Trans., 7B (1976) , 443.
5 諏訪正輝;小室滕博;添野浩,日本金属学会誌,40 (1976) ,1074.
6 赵惠田;纪士辰;王国志;魏向东,摩擦磨损,2 (1984) ,17.
7 Rohatgi, P.K.: Murachi. N.: Sherry, H.R.; Chandrashekhar, R.. Mater. Sci. Eng., 26 (1976) , 115.
8 Pai, B. C.: Rohatgi, P.K.: Venkatesh, S., Wear, 30 (1974) , 117.
9 Badia. F.A.: Rohatgi, P.K., Trans. SAE. 78 (1969) , 1200.
10 铸造有色合金手册编写组,铸造有色合金手册,机械工业出版社,1978年,p.113.
11 纪士辰;王国志;赵惠田,机械工程材料,8(1984) ,№ 4,53.~
No related articles found!
No Suggested Reading articles found!