CRYSTALLINE STRUCTURE AND TWIN OF Cr_7 C_3 IN SUPERALLOYS
LI Yuqing; LIU Jinyan (Research Institute of Daye Steel Works)
Cite this article: 

LI Yuqing; LIU Jinyan (Research Institute of Daye Steel Works). CRYSTALLINE STRUCTURE AND TWIN OF Cr_7 C_3 IN SUPERALLOYS. Acta Metall Sin, 1986, 22(1): 50-63.

Download:  PDF(1938KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Experimental confirmation by analysis of single crystal electron diffraction spots is presented, showing that the Cr_7C_3 in superalloys is of the orthorhombic crystalline structure. In the Cr_7C_3, the {013} growth twin was discovered by the electron diffraction patterns and the secondary twin might be possibly found. The {013} twin is observed in Cr_7C_3 film. The interrelation of higher twin in Cr_7C_3 has also been discussed.
Received:  18 January 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I1/50

1 Westgren, A., Jernkontorets Ann., 119 (1935) , 231.
2 Herbstein, F.H.; Snyman, J.A., Inorg. Chem., 3 (1964) , 894.
3 Fyuchart, R.; Senateur, J.-P.; Bouchaud, J.-P,; Michel, A., C.R. Hebd. Seances Acad. Sci., 260 (1965) , 913.
4 Fruchart, R.; Rouault, A., Ann. Chim., (Paris), 4 (1969) , 143.
5 桶谷繁雄,電子線回折金属炭化物研究,株式会社,东京,1971,p.217. 259.M
No related articles found!
No Suggested Reading articles found!