Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (6): 77-82    DOI:
Current Issue | Archive | Adv Search |
SIMULATION OF HEAT TRANSFER BY WATER SPRAY COOLING DURING CONTINUOUS CASTING OF LOW CARBON STEEL
by ZHANG Keqiang;YUAN Weixia;CAI Kaike Beijing University of Iron and Steel Technology
Cite this article: 

by ZHANG Keqiang;YUAN Weixia;CAI Kaike Beijing University of Iron and Steel Technology. SIMULATION OF HEAT TRANSFER BY WATER SPRAY COOLING DURING CONTINUOUS CASTING OF LOW CARBON STEEL. Acta Metall Sin, 1985, 21(6): 77-82.

Download:  PDF(402KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A simulation of heat transfer from the water droplet sprayed over the hotsurface of low carbon steel bar of continuous casting has been made. The distri-bution of water spray flux density of full cone nozzles and the heat transfercoefficient have been determined. The surface temperature of casting steel bar, thewater spray flux density and the speed of water droplets as well as others in-fluenced on the heat transfer coefficient have also been discussed.
Received:  18 June 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I6/77

1 Mizikar, E. A., Iron Steel Eng., 47 (1970) . № 6. 53.
2 Muller. H.; Jeschar, R., Arch. Eisenhuettenwes., 44 (1973) , 589.
3 Lambert. N.; Economopoulos, M., J. Iron Steel Inst., 208 (1970) , 917.
4 Bolle, L.; Moureau. J. C., Heat and Mass Transfer in Metallurgical Systems, Thesis of Seminar of ICHMT, Sept., 1979, p. 527.
5 Araki, K.; Moriyama. A.; Terada, K.; Mori. S., Trans. Iron Steel Inst. Jpn., 20(1980) . 462.
6 蔡开科;刘凤荣,金属学报,20(1984) ,B147.
No related articles found!
No Suggested Reading articles found!