SURFACE TENSION OF LIQUID Ni-P AND Ni-Zr-P ALLOYS AND THEIR WETTABILITY ONTO ALUMINA
by WANG Jingtang;CHEN Qiu;YU Yongtian;LI Gusong Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

by WANG Jingtang;CHEN Qiu;YU Yongtian;LI Gusong Institute of Metal Research; Academia Sinica; Shenyang. SURFACE TENSION OF LIQUID Ni-P AND Ni-Zr-P ALLOYS AND THEIR WETTABILITY ONTO ALUMINA. Acta Metall Sin, 1985, 21(6): 65-72.

Download:  PDF(613KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The surface tension of liquid Ni-P and Ni-Zr-P alloys and their wettabilityonto Al_2O_3 substrates were measured by the sessile drop method. The distributionof P along the depth beneath the surface of the alloy was determined by AES.Results show that the P is a surface-active element in liquid Ni and the surfacetension of liquid Ni-base alloy is obviously decreased by the increasing of P con-tained when a small amount of Zr existed. The maximum adsorption value ofP on the liquid Ni surface is rather close to the measured value by AES. Thewettability of Iiquid Ni-P onto Al_2O_3 is concerned with the P content in the all-oys and decreases as less Zr contained in them. The apparent shearing strengthof the Ni-base alloys against Al_2O_3 substrate was also evaluated.
Received:  18 June 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I6/65

1 Allen, B. C., Liquid Metals-Chemistry and Physics, Ed. Beer, S. Z., Marcel Dekker, Inc., New York, 1972, p. 161.
2 (王景唐);(1960) ,№ 1,30.
3 Humenik, M.; Kingery W. D., J. Am. Ceram. Soc., 37(1954) , 18.
4 Wilson, J. R., Metall. Rev., 10(1965) , 381
5 门间改三;须藤一;日本金属学会志,24(1960) ,167,611,163.
6 获野和已;泰松齐,日本金属学会志,43(1979) ,871.
7 Allen, B. C.; Kingery. W. D., Trans Metall. Soc AIME, 215(1959) , 30.
8 荻野和已;泰松齐;中谷文忠,日本金属学会志,46(1982) ,1049.
9 冶金部有色金属研究总院氩气组,稀有金属,4(1982) ,34.
10 Bashforth, F.; Adams, J. C., An Attempt to test the Thories of Capillary Action, Cambridge Univ., London, 1883, p. B1--26.
11 王景唐;边茂恕;马路铭,待发表。
12 Nicholas, M.; Forgan, R. R. D.; Poole, D, M., J. Mater. Sci., 3(1968) , 9.
13 Davis, L. E.; MacDanald, N. C.; Palmberg, P. W.; Riach, G. E.; Weber, R. E., Handbook of Auger Electron Spectroscopy, 2nd ed., Ed. Palmberg, P. W., Phys. Electr. Ind., 1976.
14 陈世朴;王永瑞,金属电子显微分析,机械工业出版社,北京,1982,p.226.
15 (王景唐);(1960) , № 2, 49.
16 Pask, J. A.; Futrath, R. M., J. Am. Ceram. Soc., 45(1962) . 592.
17 王景唐,金属学报,8(1965) , 59.
18 Kingery, W. D., J. Am. Ceram. Soc., 37(1954) . 42.
No related articles found!
No Suggested Reading articles found!