| SOME THERMODYNAMIC PROPERTIES IN PROCESS OF THERMAL REDUCTION OF Mg WITH HIGH AI ALLOY |
| by CAO Rongjiang;LI Guoxun;WU Xianxi Beijing General Research Institute of Non-Ferrous Metals |
|
Cite this article:
by CAO Rongjiang;LI Guoxun;WU Xianxi Beijing General Research Institute of Non-Ferrous Metals. SOME THERMODYNAMIC PROPERTIES IN PROCESS OF THERMAL REDUCTION OF Mg WITH HIGH AI ALLOY. Acta Metall Sin, 1985, 21(6): 59-64.
|
|
|
Abstract The vapour pressure of Mg, P_(Mg), over their thermal reduction of Mg withreducing agent, a high Al alloy containing Si 18.9% and Fe 5.1%, at varioustemperatures was measured by the transportation method as:lg P_(Mg)=-8853/T+10.58As compared with ferrosilicon as reducing agent, the reduction temperature maybe reduced about 200℃ at the same P_(Mg). The activity of each component inAl-Si-Fe alloy at various temperatures was calculated using the data measured byboth Bonnier method and this study. The activities of all components in theternary system have negative deviations, especially, very high for Fe. Based onthe above-mentioned data of the activities, the equilibrium constant and enthalpyof the reduction were also calculated as follows:lg K_[Al]=-18.4×10~4/T+117.2△H=3529.5 kJ
|
|
Received: 18 June 1985
|
1 Crjotheim. K., Can. J. Chem,. 39 (1961) , 2290. 2 Pidgeon. L. M., Can. Metall. Q., 10(1971) , 109. 3 Mitani. H.; Nagai. H., J. Jpn. Inst. Light Met., 21 (1971) . 648. 4 Schuhmann, R., Jr., Acta Metall., 3(1955) , 219. 5 Bonnier. E.; Caboz, R., C. R. Hebd. Seances Acad. Sci., 250(1960) , 507. 6 Darken, L. S., Trans. Metall. Soc. AIME, 239 (1967) . 82. 7 51(1977) , 495. 8 Mitani, H.; Nagai. H., J. Jpn. Inst. Met., 31(1967) , 1296. 9 小松童选,日本矿业会志,77(1961) ,67. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|