CALCULATION OF ACTIVITIES IN In-As AND Ga-As SYSTEMS
WU Jisen;ZOU Yuanxi(Chou Yuanhsi);MO Peigen Shanghai Institute of Metallurgy;Academia Sinica
Cite this article: 

WU Jisen;ZOU Yuanxi(Chou Yuanhsi);MO Peigen Shanghai Institute of Metallurgy;Academia Sinica. CALCULATION OF ACTIVITIES IN In-As AND Ga-As SYSTEMS. Acta Metall Sin, 1985, 21(5): 74-84.

Download:  PDF(774KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A criterion for ascertaining the accuracy of the free energy of formation ofan intermetallic compound has been obtained from a combination of the modifiedGibbs-Duhem equation,the function transformation and the phase diagram.Thefree energies of formation of InAs and GaAs have been selected on the basis ofthe above-mentioned criterion.The activities in the binary In-As and Ga-As sys-tems are then calculated by means of the modified Gibbs-Duhem equation in con-junction with the properly chosen free energies of formation of the compoundsInAs and GaAs and the binary In-As and Ga-As phase diagrams.
Received:  18 May 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I5/74

1 Vieland,L.,Acta Metall.,11(1963) ,137.
2 Richman,D.,J.Phys.Chem.Solids,24(1963) ,1131.
3 Thurmond,D.,J.Phys.Chem.Solids,26(1965) ,785.
4 Arthur,J.R.,J.Phys.Chem.Solids,28(1967) ,2257.
5 Panish,M.B.,J.Cryst.Growth,27(1974) ,6.
6 Stringfellow G.B.;Greene,P.E.,J.Phys.Chem.Solids,30(1969) ,1779.
7 Osamura,K.;Murakami,Y.,J.phys.Chem.Solids,36(1975) ,931.
8 Peuschel,G.-P.;Apelt,R.;Knoblock,G.;Butter,E.,Krist.Tech.,14(1979) ,409.
9 Knobloch,G.;Butter,E.;Reiffarth,S.,Z.Phys.Chem.,259(1978) ,667.
10 Brebrick,R.E.,Metall.Trans.,8A(1977) ,403.
11 邹元熾,金属学报,7(1964) ,123.
12 周国治,金属学报,8(1965) ,545.
13 Hansen,M.,Constitutions of Binary Alloys,2nd ed.,McGraw-Hill,1958,p.167.
14 Liu,T.S.;Peretti,E.A.,Trans.ASM,44(1952) ,539.
15 Van Den Boomgaard,J.;Schol,K.,Philips Res.Rep.,12(1957) ,127.
16 Hall,R.N.,J.Electrochem.Soc.,110(1963) ,385.
17 #12
18 #12
19 Stull,D.R.;Sinke,G.C.,Thermodynamic Properties of the Elements,Am.Chem.Soc.,(1956) .
20 Hultgren,R.;Desai,P.D.;Hawkins,D.T.;Gleiser,M.;Kelley,K.K.;Wagman,D.D.,Selected Values of the Thermodynamic Properties of the Elements.ASM Metals Park,Ohio,1973.
21 Lichter,B.D.;Sommelet,P.,Trans.Metall.Soc.AIME,245(1969) ,1021.
22 Pupp,C.;Murrey,J.J.;Pottie,R.E.,J.Chem.Thermody.,6(1974) ,123.
23 Horiba,S.,Z.Phys.Chem.,106(1923) ,295.
24 Barin,I.;Knacke.O.,Thermochemical Properties of Inorganic Substances,Berlin,Springer-Verlag,1977,p.43.
25 #12
26 #12
27 伊藤聪;日野光久;阿座上竹四,日本金属学会志,46(1982) ,162.
No related articles found!
No Suggested Reading articles found!