Acta Metall Sin  1985, Vol. 21 Issue (5): 128-136    DOI:
Current Issue | Archive | Adv Search |
COMPUTER SIMULATION OF CRYSTAL PROJECTION AND DIFFRACTION PATTERN
PAN Jinsheng Tsinghua University;Beijing
Cite this article: 

PAN Jinsheng Tsinghua University;Beijing. COMPUTER SIMULATION OF CRYSTAL PROJECTION AND DIFFRACTION PATTERN. Acta Metall Sin, 1985, 21(5): 128-136.

Download:  PDF(545KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the gnomonic projections and on the rotational reciprocal coordi-nate axes,a computer program,written in BASIC,is compiled for the simulationof various kinds of projections and diffraction patterns of crystals.These includethe standard gnomonic and stereographic projections,the transmission and back-reflection Laue patterns and the electron diffraction patterns.The projections anddiffraction patterns of both matrix and twin can be drawn together.In the caseof electron diffraction,the pattern may contain spots on any reciprocal layer be-sides the zero one.It is shown that these projections and patterns can be conve-niently used for the indexing of the diffraction spots and the determination of thecrystal symmetry,the type of the twin and the orientation relationship betweenmatrix and twin.
Received:  18 May 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I5/128

1 许顺生,金属X射线学,上海科技出版社,1962 p.223.
2 Goehner,R.P.,Advances in X-Ray Analysis,Vol.19,Ed.Gould.R.W.;et al.Kendall/Hunt Publ.,Dubugue,Lowa,1976,p.725.
3 Smaill,J.S.,Metallurgical Sterographical Projections,Adam Hilger,London,1972,p.63.
4 Preuss,E.;Krahl-Urban,B.;Butz,R.,Laue Atlas,Berlelsmann Universitaetsverlag,Germany,1974.
5 潘金生,金属学报,18(1982) ,703.
6 Jaswon,M.A.;Dove,D.B.,A(?)t(?) Crystallogr.,9(1956) ,621.
No related articles found!
No Suggested Reading articles found!