CARBIDE PARTICLE CRACKING IN SPHEROIDIZED CARBON STEELS
ZHANG Yizeng;LIU Xiangjie Huazhong University of Science and Technology;Wuhan
Cite this article: 

ZHANG Yizeng;LIU Xiangjie Huazhong University of Science and Technology;Wuhan. CARBIDE PARTICLE CRACKING IN SPHEROIDIZED CARBON STEELS. Acta Metall Sin, 1985, 21(4): 57-62.

Download:  PDF(488KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A quantitative study of the carbide particle cracking was performed on fourdifferent spheroidized carbon steels deformed uniaxially in tension.The local crit-ical stresses for the carbon particle cracking were estimated.Based on these obser-vations and computations,the effect of microstructure on the carbide particlecracking was also discussed.
Received:  18 April 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I4/57

1 Argon,A.S.;Im,J.;Safoglu,R.,Metall.Trans.,6A(1975) ,839.
2 Fisher,J.R.;Guriland,J.,Met.Sci.,15(1981) ,193.
3 Lc Roy,G.;Embury,J.D.;Edward,G.;Ashby,M.F.,Acta Metall.,29(1981) ,1509.
4 张以增,金属学报,19(1983) ,A70.
5 Zou,H.-C.;Lou,Y.-L.;Zhang,Y.-Z.,Met.Sci Eng.,62(1984) ,163.
6 Gurland,J.,Acta Metall.,20(1972) ,735.
7 Inoue,T.;Kinoshita,S.,The Microstructure and Design of Alloys,Proc.of the 3rd Int.Conf.on the Strength of Metals and Alloys,Cambridge,England,Aug.20,1973,Sponsored by The Inst.of Metals and The Iron and Steel Inst.,Vol.1,paper 32,1973,p.159.
8 Needleman,A.,J.Mech.Phys.Solids,20(1970) ,111.
9 McCormick,C.W.,NASTRAN Users Manual,Level 15. 5,Document NASA ST[(222) 01] ,NASA,Washington,DC.,1973.
10 Kelly,A.,Strong Solids,Oxford Univ.Press,1966,p.9
No related articles found!