Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (4): 13-20    DOI:
Current Issue | Archive | Adv Search |
THE CARBONITRIDE IN GAS CARBONITRIDING LAYER ON 18CrMnNiMoA STEEL
NIE Changshen;CHONG Keduan;ZHANG Cunxin;YAO Jingfu Nei Monggol Institute of Metallic Materials
Cite this article: 

NIE Changshen;CHONG Keduan;ZHANG Cunxin;YAO Jingfu Nei Monggol Institute of Metallic Materials. THE CARBONITRIDE IN GAS CARBONITRIDING LAYER ON 18CrMnNiMoA STEEL. Acta Metall Sin, 1985, 21(4): 13-20.

Download:  PDF(1532KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The properties of gas carbonitriding layer on 18CrMnNiMoA steel relatingto its morphology,structure,composition,distribution and partition of alloyingelements among the phases contained have been studied by means of electrolyticextraction-chemical separation-X-ray diffraction phase analysis layer by layer,aswell as by TEM or electron diffraction observation and by chemical analysis.Thestrengthening mechanism of the carbonitriding layer has also been discussed.
Received:  18 April 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I4/13

1 淹岛延雄,金属材料,12(1972) ,№4,27.
2 Jack,K.H.,Heat Treatment,The Metals Society,London,1975,p.39.
3 #12
4 尹雪峰;朱敦伦;石大庆,金属热处理,(1984) ,№1,31.
5 雷天同;赵鹏文;陈庆福;荆小龙,金属热处理,(1984) ,№7,13.
6 聂常绅;刘宏凯,分析化学,11(1983) ,№3,197.
7 聂常绅;陈学军;韩利华,冶金分析与测试,冶金分析分册,4(1984) ,№1,15.
8 若松茂雄,铁钢,55(1969) ,1359.
9 聂常绅,理化检验,化学分册,(1977) ,№3-4,1.
10 吉松史郎;荒木透;中川龙一,铁钢,54(1968) ,936.
11 今井勇之进;增本健;前田启吉,日本金属学会志,29(1965) ,866.
12 Imai Yunoshin;Masumoto Tsuyoshi;Maeda KeikichioSci.Rep.Res.Inst.,Tohoku Univ.,A19(1967) ,35.
13 增本健;今井勇之进;奈贺正明,日本金属学会志,33(1969) ,705.
14 增本健;今井勇之进,日本金属学会志,33(1969) ,927.
15 高濑孝夫,金属材料,12(1972) ,№4,16.
16 #12
17 郭可信,金属学报,2(1957) ,303.
18 房荣富;韩连香,金属材料与热加工工艺,(1981) ,№2-3,129.
No related articles found!