DETERMINATION OF σ-OR M_(23)C_6-PHASE IN STAINLESS STEEL BY STEP POTENTIAL ETCHING CURRENT METHOD
MA Xiang Central Iron and Steel Research Institute;Ministry of Metallurgical Industry;Beijing
Cite this article: 

MA Xiang Central Iron and Steel Research Institute;Ministry of Metallurgical Industry;Beijing. DETERMINATION OF σ-OR M_(23)C_6-PHASE IN STAINLESS STEEL BY STEP POTENTIAL ETCHING CURRENT METHOD. Acta Metall Sin, 1985, 21(4): 128-138.

Download:  PDF(1493KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new method,namely,the step potential etching current mehtod for theindividual determination of σ-or M_(23)C_6-phase which is a difficult problem to sepa-rate each other by conventional chemical manner has been developed.This simpli-fied and rapid method easy to give certain information about the composition,con-tent and morphology of precipitated phases in the steel has been applied to stain-less steel samples.In addition,a formula for quantitative analysis was derived onthe basis of a new model of electrode process.The formula has been confirmedby experiments.
Received:  18 April 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I4/128

1 #12
2 #12
3 #12
4 #12
5 #12
6 #12
7 斋田义幸;筒井光范,日本金属学会志,42(1978) ,769.
8 马翔 徐澄宇;钢铁研究总院学报,4,(1984) ,№1,114.
9 马翔,分析化学,12(1984) ,№6,495.
10 马翔,分析化学,12(1984) ,№1,1.
11 黑泽文夫;田口勇;松本龙太郎,日本金属学会志,43(1979) ,1068.
12 Nicholson,R.S.;Shain,I.,Anal.Chem.,36(1964) ,706.
No related articles found!
No Suggested Reading articles found!