INFLUENCE OF TRANSITION METALS OF THE THIRD LONG PERIOD ON DUCTILE-BRITTLE TRANSFORMATION OF PdSi_(16.5)GLASS
ZHENG Yun;NING Yuantao Institute of Precious Metals;Kunming
Cite this article: 

ZHENG Yun;NING Yuantao Institute of Precious Metals;Kunming. INFLUENCE OF TRANSITION METALS OF THE THIRD LONG PERIOD ON DUCTILE-BRITTLE TRANSFORMATION OF PdSi_(16.5)GLASS. Acta Metall Sin, 1985, 21(4): 113-119.

Download:  PDF(536KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The stress relief and ductile-brittle transformation of the metallic glasses Pd_(82.5)M_1Si_(16.5)prepared by spinning roll have been examined.It was found that theductile-brittle transformation temperature,T_B,and activation energy,△E_B,of theglasses composed by the preceding transition metals,e.g.,Hf,Ta,W,Re,are in-creased markedly and by the later ones,e.g.,Os,Pt,influenced slightly,but byIr,T_B is decreased too many.The mode of ductile-brittle transformation of themetallic glasses PdSi_(16.5)is different among themselves composed by the precedingand later transition metals.The comparison of the influences of additives on theirtemperatures and activation energies of the ductile-brittle transformation and glasstransition has been made.These behaviours have been discussed on the basis ofthe Gaskell′s model and the Engel-Brewer′s electron theory of transition metals.
Received:  18 April 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I4/113

1 Walter,J.W.;Luborsky,F.E.,Mater.Sci Eng.,33(1978) ,91.
2 Liebermann,H.H.;Luborsky,F.E.,Acta Metall.,29(1981) ,1413
3 宁远涛;郑云;祁更新,金属学报,19(1983) ,B 209.
4 Luborsky,F.E.;Walter,J.L.,J.Appl.Phys.,47(1976) ,3648.
5 Masumoto,T.;Maddin,R.,Acta Metall.,19(1971) ,725.
6 Chen,H.S.,J.Non-Crystal Solids,27(1978) ,257.
7 Chen,H.S.,Mater.Sci.Eng.,26(1976) ,79.
8 Freed,R.L.;Vander Sande,J.B.,Acta Metall.,28(1980) ,103.a
No related articles found!
No Suggested Reading articles found!