Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (4): 105-112    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF Cr,Mo OR W ADDITION ON MAGNETIC PROPERTIES OF AMORPHOUS Fe-B ALLOYS
ZHAN Wenshan;SHEN Baogen;ZHAO 2iangao;PAN Xiaoshuo Institute of Physics;Academia Sinica;Beijing
Cite this article: 

ZHAN Wenshan;SHEN Baogen;ZHAO 2iangao;PAN Xiaoshuo Institute of Physics;Academia Sinica;Beijing. EFFECT OF Cr,Mo OR W ADDITION ON MAGNETIC PROPERTIES OF AMORPHOUS Fe-B ALLOYS. Acta Metall Sin, 1985, 21(4): 105-112.

Download:  PDF(606KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Experimental results for atomic magnetic moment,Curie temperature,T_C,andcoefficient B of the T~(3/2)term in the Bloch law for amorphous alloys Fe-M-B(M=Cr,Mo or W)prepared by the drum spinning technique are reported.Theaverage magnetic moment for each metal atom is 2.0,-3.96,-4.62 or -4.08μ_B for Fe,Cr,Mo or W respectively in the three amorphous alloy systems.Thedecrease of T_C is at the rate of 20.5K/at.-% Cr,27.7K/at.-% Mo,or 26K/at.-%W with increasing Cr,Mo or W content respectively.These results are discussedin the light of a‘mixed’model due to C.W.Chen.The effect of the magneticshort range order around T_C is clearly observed by applying an external magneticfield.The coefficient B increases with the concentration of Cr,Mo or W,whichis interpreted as a consequence of weakening of exchange coupling between themagnetic atoms.
Received:  18 April 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I4/105

1 Mizoguchi,T.;Yamauchi,K.;Miyajima,H.,Amorphous Magnetism,Ed Hooper and de Graaf,Plenum Press,New York,1973,p.325.
2 Dey,S.;Gorres,U.;Nielsen,H.J.V.;Rosenbery,M.;Sostarich,J.J.Phys.(Paris),41(1980) ,C8-675.
3 Nielsen,H.J.V.,J.Magn.Magn.Mater.,12(1979) ,187;19(1980) ,138.
4 Nielsen,H.J.V.,Solid State Commun.,30(1979) ,239.
5 詹文山,物理,11(1982) ,732.
6 Chen,C.W.,Magnetism and Metallurgy of Soft Magnetic Materials,North-Holland Publishing Company Amsterdam,New York,1977,p.200.
7 Friedel,J.,Nuovo Cimento,Suppl.,7(1958) ,200.
8 近角聪信,强磁性体物理(上),裳华房,1978,p.182.
9 Chen,H.S.;Sherwood,R.C.;Leamy,H.J.;Gyorgy,E.M.,IEEE Trans.Magn.,MAG-12(1976) ,933.
10 Kazama,N.;Kameda,M.;Masumoto,T.,AlP Conf.Proc.34(1976) ,307.
11 Chien.C.L.;Hasegawa,R.,J.Appl.Phys.,49(1978) ,1721.
12 郭贻诚;铁磁学,高等教育出版社,1965,p.88.
No related articles found!