Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (2): 88-91    DOI:
Current Issue | Archive | Adv Search |
A PART OF ROOM TEMPERATURE SECTION OF PHASE DIAGRAM OF Y-Cu-Ni(Y≤16.7 at.-%)SYSTEM
ZHENG Jianxuan Guangxi University;NONG Liangqin Guangxi Institute for Nationalities
Cite this article: 

ZHENG Jianxuan Guangxi University;NONG Liangqin Guangxi Institute for Nationalities. A PART OF ROOM TEMPERATURE SECTION OF PHASE DIAGRAM OF Y-Cu-Ni(Y≤16.7 at.-%)SYSTEM. Acta Metall Sin, 1985, 21(2): 88-91.

Download:  PDF(250KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The room temperature section of the phase diagram of the ternary Y-Cu-Nisystem for Y≤16.7 at.-% has been determined by X-ray powder diffractionmethod.Four single-phase regions:α,β,ε and ω;five two-phase regions:α+β,α+ε,α+ω,β+ω and ε+ω;and two three-phase regions:α+β+ω and α+ε+ωare found in the section.X-ray analysis showed that maximum solubility of Y inα-phase is about 2 wt-%.
Received:  18 February 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I2/88

1 Shaltiel,D.;Wernick,J.H.;Williams,H.J.;Peter,M.,Phys.Rev.,135(1964) ,A1358.
2 Domagula,R.,F.;Rausch,J.J.;Levinson,Do W.,Trans.ASM,53(1961) ,150.
3 Wernick,J.H.;Geller,S.,Acta Cryst.,12(1959) ,662.
4 Buschow,K.H.J.;Van Der Goot,A.S.,Acta Cryst.,B27(1971) ,1087.
5 Gschneidner,K.A.,Jr.,Rare Earth Alloys,D.Van Nostrand Company Inc.,Princeton,New Jersy,1961,p.160.
6 Chuang,Y.C.;Wu,C.H.;Chang,Y.C.,J.Less-Common Met.,84(1982) ,204.
7 Beaudry,B.J.;Daane,A.H.,Trans.Metall.Soc.AIME,218(1960) ,854.
8 Hansen,M.;Anderko,K.,Constitution of Binary Alloys,McGraw-Hill,New York,1958,p.601.-