THE m-C-δ OR m-k-δ RELATIONS OF SUPERPLASTICITY OF Zn-5%Al EUTECTIC ALLOY
LIU Qin(Chin Liu);XIA Chu;LIU Xiaodong Shanghai Jiaotong University
Cite this article: 

LIU Qin(Chin Liu);XIA Chu;LIU Xiaodong Shanghai Jiaotong University. THE m-C-δ OR m-k-δ RELATIONS OF SUPERPLASTICITY OF Zn-5%Al EUTECTIC ALLOY. Acta Metall Sin, 1985, 21(2): 111-117.

Download:  PDF(1331KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The m-C-δ or m-k-δ relations(simply called m-δ relation)have been obtainedfor the Zn-5%Al eutectic alloy with three average strain rates:3.7×10~(-2),7.4×10~(-2)and 1.1×10~(-1) min~(-1),at five temperatures:170,190,210,230 and 250℃.It was found that all m values increased rapidly with the increase in strainat the start,till a certain strain,called limit strain,was reached and then decreasedslowly and remained steady till fracture.A peak m value corresponding to the limitstrain may be found on each curve.The equation suggested by one of the authorscan apply to this alloy and all C values including C_I and C_F has been calculatedfor every point on all m-C-δ or m-k-δ curves.The plots of relations of C vs δ arenearly straight lines.The slopes of these lines fall suddenly at the limit strain.
Received:  18 February 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I2/111

1 Backofen,W.A.;Iurner,I.R.;Avery,D.H.;ASM Trans.Q.,57(1964) ,980.
2 Avery,D.H.;Backofen,W.A.,ASM Trans.Q.,58(1965) ,551.
3 刘勤,上海交通大学学报,(1982) ,№2,125.
4 刘勤,上海交通大学学报,(1983) ,№1,127.
5 刘勤,塑性と加工,24(1983) ,№270,692.
6 刘勤;李寿民,上海交通大学学报,(1984) ,№1,129.
7 刘勤;李寿民,上海交通大学学报,(1984) ,№4.
8 李寿民;刘勤,“一个测恒定真应变速率的简便方法(变υ-定ε法),上海市金属学会,有色金属专业委员会,1983年年会论文.
No related articles found!
No Suggested Reading articles found!