EFFECT OF Fe CONTENT ON STRENGTHENING OF ELECTRICAL CONDUCTIVE Cu-Fe ALLOY
JIANG Hancheng Jilin University;Changchun
Cite this article: 

JIANG Hancheng Jilin University;Changchun. EFFECT OF Fe CONTENT ON STRENGTHENING OF ELECTRICAL CONDUCTIVE Cu-Fe ALLOY. Acta Metall Sin, 1985, 21(2): 1-5.

Download:  PDF(976KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A study was conducted to obtain a better understanding of the effect of Fecontent on strengthening of the super strength electrical conductive Cu-Fe alloy.Under certain specified technique with Fe content about 10 at.-%,the electricalconductivity of the alloy may be up to 59—60%(IACS)and the ultimate stregthup to 6.4×10~2 MN/m~2 as well.When the Fe content over 10 at.-%,its strengthraises linearly with Fe content.It is proposed that the strengthening is mainlycaused by the fibre reinforcement of even distributed α-phase in the alloy matrixof ε-phase as a composite material.
Received:  18 February 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I2/1

1 粟田昌良;白鸟元已,金属,41(1971) ,№ 18,83.
2 河野纪雄;姜汉成;丹博司;室町繁雄;渡边久藤,伸铜技术研究会志,22(1983) ,59.
3 Hansen,M.,Constitution of Binary Alloys,McGraw-Hill,New York,1958,580.
4 Kelly,A,Strong Solids,2nd ed.,Clarendon Press,Oxford,1973,p.157.
5 井形直弘;佐东信司,Cu-Fe合金强化(?)关(?)研究,(待发表).
6 姜汉成,机械工程材料,8(1984) ,№ 2 76.
7 村上阳太郎,纤维强化金属材料(?)现状(?)问题点,关西大学院特别讲义,1981. p.5
No related articles found!
No Suggested Reading articles found!