Please wait a minute...
Acta Metall Sin  1984, Vol. 20 Issue (6): 475-482    DOI:
Current Issue | Archive | Adv Search |
REDUCTION RATE OF FeO IN MOLTEN SLAG BY SOLID CARBON
ZHOU Yusheng (Ma'anshan Institute of Iron and Steel Technology); DU Ting (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 31 January; 1983; revised manuscript 9 February; 1984)
Cite this article: 

ZHOU Yusheng (Ma'anshan Institute of Iron and Steel Technology); DU Ting (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 31 January; 1983; revised manuscript 9 February; 1984). REDUCTION RATE OF FeO IN MOLTEN SLAG BY SOLID CARBON. Acta Metall Sin, 1984, 20(6): 475-482.

Download:  PDF(561KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The reduction rate of FeO in molten slags of two systems FeO-CaO-SiO_2-MgO and FeO-CaO-SiO_2 by solid carbon has been determined by the method of measuring the kinetic parameters in which a combination of the initial concentration in system with the weightless rate of reductant in the reaction process was made. The reduction rate determined by this study is of an apparent first order reaction of overall wt-% of FeO. The measured apparent activation energy is 222.60 kJ/mol. The empirical equation of the rate is v=-(W_s/A)dc/dt=1453.0[exp(222600/RT)]·C Experimental results show that the convection diffusion is the rate-controlling step in the reduction of molten FeO by solid carbon.
Received:  18 June 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I6/475

1 佐佐木康;岡本恭典;相马胤和,鉄鋼,64(1978) ,367.
2 Davies, M. W.; Hazeldean, G. S. F; Smith, P. N., Physical Chemistry of Process Metallurgy, The Richardson Conference, Eds. Jeffes, J. H. E.; Tait, R. J., Inst. Min. Metall, 1974; p.95.
3 Krainer, H.; Beer, H.P.; Brandl, H., Tech. Mitt. Krupp, Fors chungsber., 24 (1966) , 139.
4 Fay Fun, Metall. Trans., 1(1970) , 2537.
5 须贺田正泰;杉山喬,近藤真一,鉄鋼,58(1972) ,1363.
6 Frost, A. A.; Pearson, R. G.化学动力学和历程--均相化学反应的研究,孙承谔译,科学出版社,1966,p.9-50.
7 魏寿昆,冶金过程热力学,上海科学技术出版社,1980,p.233.
8 Wagner, C., The Physical Chemistry of Steelmalcing, Ed. Elliott, J. F., Wiley, New York, 1958, p. 237.
9 1956, p. 284.
10 王渭源,金属学报,7(1964) ,376.
11 Richardson, F. D., Steelmalcing, The Chipman Conference, Eds. Elliott, J. F.; Meadowcroft, R., Cambridge, Mass, MIT, 1962, p.66.
No related articles found!