HYDROGEN ABSORPTION OF LaNi_xAl_y ALLOYS
QIAN Jiuxin; ZHAO Liming; ZHENG Chaogui; YE Yupu (Department of Chemistry; Peking University. Beijing) (Manuscript received 15 September; 1983; revised manuscript 9 February; 1984)
Cite this article: 

QIAN Jiuxin; ZHAO Liming; ZHENG Chaogui; YE Yupu (Department of Chemistry; Peking University. Beijing) (Manuscript received 15 September; 1983; revised manuscript 9 February; 1984). HYDROGEN ABSORPTION OF LaNi_xAl_y ALLOYS. Acta Metall Sin, 1984, 20(6): 423-428.

Download:  PDF(408KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  X-ray diffraction analysis was used to ascertain the LaNi_5-base solid solution range in the La-Ni-Al ternary system This range at 800℃ was found to be Al< 12.2 and 31
Received:  18 June 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I6/423

1 Van Mal, H. H.; Buschow, K. H. J.; Miedema, A. R., J. Less-Common Met., 35 (1974) , 65.
2 Mendelsohn, M. H.; Gruen, D. M.; Dwight, A. E., The Rare Earth in Modern Science and Technology, Eds. McCarthy, G. J.; Rhyne, J. J., Plenum Press, New York, 1978, p. 25.
3 Achard, J. C.; Percheron-Guegan, A.; Diaz, H.; Briaucourt, F.; Demany, F., Hydrogen in Metall, Vol.2, Proc. of the 2nd Int. Congress, Held at Paris, June 1977, Behalf of the Int. Association for Hydrogen Energy, Paris, 1977, p. 1El2.
4 Dwight, A. E., The Rare Earth in Modern Science and Technology, Eds. McCarthy, G. J.; Rhyne, J. J., Plenum Press, New York, 1978, p. 325.+
No related articles found!
No Suggested Reading articles found!