| NOTE ON B AND M_3B_2 IN A NiFeCrWMoTiAl ALLOY |
| LI Yuqing (Research Institute of Daye Steel Works)(Manuscript received S July; 1983; revised manuscript 13 December; 1983) |
|
Cite this article:
LI Yuqing (Research Institute of Daye Steel Works)(Manuscript received S July; 1983; revised manuscript 13 December; 1983). NOTE ON B AND M_3B_2 IN A NiFeCrWMoTiAl ALLOY. Acta Metall Sin, 1984, 20(5): 329-452.
|
|
|
Abstract An electron microscope study was made of the effect of B, especially as M_3B_2, on a NiFeCrWMoTiAl alloy using the fractograph of extraction carbon replica. The B additive may decrease and dissipate the, brittle flakes of Ti_4C_2S_2 which ordinarily embrittle the alloy without any B along the grain boundaries. The M_3B_2 was observed in the shape of flakes or dendritic flakes and of blocks in the alloys containing 0.025—0.050 and 0.075—0.100% B respectively. During heating under temperature below 1200℃, the M_3B_2 grains precipitate and the flaky M_3B_2 transforms into grains as well.
|
|
Received: 18 May 1984
|
1 Decker, R. F.; Sims, C. T., Superalloys, Eds. Sims, C. T.; Hagel, W. C., Wiley, New York, 1972, p. 33-77. 2 冶军编,美国镍基高温合金,科学出版社,1978. 3 郭可信,金属学报,14(1978) ,73. 4 Holt, R. T.; Wallace, W., Int. Met. Rev., 21(1976) , 1. 5 李玉清,金属学报,18(1982) ,577.J |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |