| CRYOGENIC PROPERTIES AND PARAMAGNETISMANTIFERROMAGNETISM TRANSITION OF A γ-Fe-Mn-Al ALLOY |
| ZHANG Yansheng (Institute of Metal Research; Academia Sinica; Shenyang)(Manuscript received 16 September; 1983; revised manuscript 21 December; 1983) |
|
Cite this article:
ZHANG Yansheng (Institute of Metal Research; Academia Sinica; Shenyang)(Manuscript received 16 September; 1983; revised manuscript 21 December; 1983). CRYOGENIC PROPERTIES AND PARAMAGNETISMANTIFERROMAGNETISM TRANSITION OF A γ-Fe-Mn-Al ALLOY. Acta Metall Sin, 1984, 20(5): 313-321.
|
|
|
Abstract Studies were made of the cryogenic properties, structural stability and magnetism transition of a fcc γ-Fe-Mn-Al alloy containing 25.6% Mn,4.1%Al, 0.16%C and 0.27%Si, of which the strength, ductility and austenitic stability are satisfactory at temperature range of 300 to 4 K. Its physical properties were determined as follows: lower magnetic susceptibility about 34.6×10~(-4) to 22×10~(-4) from 300 to 4 K; higher electric resistivity up to 105μΩ·cm and lower cold contraction than conventional Fe-Cr-Ni austenitic steels. A peak value is presented on the plot of temperature T dependence of magnetic susceptibility x at 320 K. The sign change of dx/dT shows the paramagnetism-antiferromagnetism transition at which an anomaly of several physical properties such as elastic modulus, heat expansion, etc. is accompanied. Furthermore, by an addition of Al to Fe-Mn alloy, its Néel temperature may be markedly lowered. The magnetic susceptibility may be increasing to a greater value at Néel temperature. In comparison with AISI 300 Cr-Ni austenitic stainless steels, the γ-Fe-Mn-Al alloy is characterized by both stable austenite and quite low magnetic susceptibility within temperature range down from 20 to 4 K. It seems to be a potential constructional material for superconducting magnet applications.
|
|
Received: 18 May 1984
|
1 张彦生,低温钢的现状、研究与发展,中国金属学会第一届特殊钢年会论文,1980,9. 2 Larbalestier, D. C.; King, H. W., Cryogenics, 13(1973) , 160. 3 Wigley, D. A., Mechanical Properties of Materials at Low Temperatures, Plenum Press, New York, 1971, p. 59. 4 Wigley, D. A., ibid., p. 89. 5 张彦生,师昌绪,金属学报,7(1964) ,285. 6 叶基石,金属学报,13(1977) ,149. 7 张彦生,金属学报,19(1983) ,A262. 8 Basinski, Z. S., Proc. R. Soc. London, Ser. A, 240(1957) , 229. 9 Honda Memorial Foundation, Physics and Applications of Invar Alloys, Maruzen Company Ltd., 1978, p. 191. 10 张彦生,γ-Fe-Mn-Al-Cr合金的顺磁性→反铁磁性转变,未发表资料,1983. 11 Abrahams, S. C.; Guttman, L; Kasper, J. S., Phys. Rev., 127 (1962) , 2052. 12 Umebayashi, H,; Ishikawa, Y., J. Phys. Soc. Jpn, 21 (1966) , 1281. 13 Ishikawa, Y.; Kongi, M.; Noda, Y., ibid., 39 (1975) , 675. 14 Endoh, Y.; Ishikawa, Y., ibid., 30 (1971) , 1614. 15 Shiga, M., ibid., 22(1967) , 539. 16 Hayase, M., ibid., 30 (1971) , 729. 17 Ledbetter, H. M.; Weston, W. F.; Naimon, E. R., J. Appl. Phys., 46 (1975) , 3855. 18 Ledbetter, H. M., Mater. Sci. Eng. 29 (1977) , 255. 19 Ledbetter, H. M., Advancesin Cryogenic Engineering, Vol. 24, Eds, Timmerhaus, K. D.; Reed, R. P.; Clark, A. F., Plenum Press, New York and London, 1978, p. 103. 20 Fujimori, H., J. Phys. Soc. Jpn, 21 (1966) , 1860. 21 Asano, S.; Yamashita, J., J. Phys. Soc. Jpn, 31(1971) , 1000. 22 Asano, S.; Yamashita, J., J. Phys. Soc. Jpn, 23(1967) , 714. 23 Warnes, L. A. A.; King, H. W., Cryogenics, 16(1976) , 659. |
| No Suggested Reading articles found! |
|
|