GUO Encai (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Belling); HAN Zhiyuan; YU Shuyou(Research Institute of Qiqihar Steel Works)(Manuscript received 17 August; 1982; revised manuscript 26 August; 1983). INFLUENCE OF Nb ON STEADY-STATE CREEP BEHAVIOUR OF Ni-Cr-Ti TYPE WROUGHT SUPERALLOY. Acta Metall Sin, 1984, 20(5): 305-312.
|
|
|
Abstract The distribution of Nb among γ, γ' and carbide phases is found to be about 5: 3: 1 in the Ni-Cr-Ti type wrought superalloy of various Nb contents. With the increasing content of Nb, the stress-exponent, n, decreases and the apparent creep activation energy, Q_(app), increases and fulfils the expression: Q_(app)=B e~(kx/lge) The grain size of the alloy and the stacking fault energy of γ matrix may be decreased by the Nb added. The steady-state creep rate, ε, obeys the following relationship: s∝L~bγ_(SFE)~α The volume fraction, the particle radius and the long range order of the γ'-phase may be also increased by the Nb added. If the effective stress(σ-σ_b) was introduced to describe the stress relationship of the steady-state creep rate, the typicalcreep equation may be: S=A_1L~bγ_(SFE)~α(σ-σ_b)~n 0exp(-(Q_(app)/RT)where σ_b is the average tensile stress opposing dislocation motion in creep. An observation on the thin foil specimens under TEM shows that the perfect dislocation α/2[10] cutting γ'-phase in glide plane (111) is resolved into two partial dislocations α/6-[11] and α/6[2]. The spacings of superlattice dislocation pairs examined are about 100—165 which fit in nearly with the measured particle size of γ'-phase.
|
|
Received: 18 May 1984
|
1 Guo, E. C.; Ma, F. J., Superalloys 1980, Proc. of the Fourth Int. Syrup. on Superalloys, Eds. Tien, J. K.; Wlodek, S. T.; Morrow, H., IlI, et al., ASM, Metals Park, Ohio, 1980, p. 431. 2 陈篪;邓枝生;吴伯群;丁树深,物理学报,23(1974) ,69. 3 Ajaja, O.; Howson, T. E.; Purushothaman, S.; Tien, J. K., Mater. Sci. Eng., 44(1980) , 165. 4 Purushothaman, S.; Tien, J. K., Acta Metall., 26(1978) , 519. 5 Marcinkowrki, M. J. et al., Acta Metall., 9(1961) , 129.E |