Please wait a minute...
Acta Metall Sin  1984, Vol. 20 Issue (4): 370-376    DOI:
Current Issue | Archive | Adv Search |
MEASUREMENT OF SURFACE TENSION OF Pb-Sb MELTS AND ITS TEMPERATURE COEFFICIENT
MA Luming; BIAN Maoshu; WANG Jingtang (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 7 March; 1983)
Cite this article: 

MA Luming; BIAN Maoshu; WANG Jingtang (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 7 March; 1983). MEASUREMENT OF SURFACE TENSION OF Pb-Sb MELTS AND ITS TEMPERATURE COEFFICIENT. Acta Metall Sin, 1984, 20(4): 370-376.

Download:  PDF(503KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Measurements of the surface tension of the Pb-Sb binary melts were made by the sessile drop method. All the temperature coefficient of their surface tension was obtained in a negative quantity. At the same measuring temperature, the values of the surface tension of Pb-Sb melts lie between that of each pure component and vary non-linearly with their compositions which show a negative diviation from the "ideal solution". As the results of this liquid binary eutectic alloy, a concept of the "liquid similar eutectic atomic clusters" (LSEAC) may be approached by the authors to interpret the surface tension phenomena of the binary alloys of eutectic type.
Received:  18 April 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I4/370

1 Olsen, D.A.; Johnson, D., J. Phys. Chem., 67 (1963) , 2529.
2 Demeri, M.; Farag, M.; Heasley, J., J. Mater. Sci., 9 (1974) , 683.
3#12
4 Bathforth, F.; Adams, J.C., An Attempt to Test the Theories of Capillary Action, Cambridge Univ. Dress, London, 1883, P. BⅡ 1-26.
5 王景唐;马禄铭;边茂恕,用卧滴法测定铅锑熔体的密度及其校正法,待发表.
6 Kirshenbaum, A.D.; Cahill, J.A.; Grosse, A.V., J. Inorg. Nucl. Chem., 22 (1961) , 33.
7 Kirshenbaum, A.D.; Cabill, J.A., ASM. Trams. Q., 55 (1962) , 849.
8 向井楠宏,日本金属学会志,37(1973) ,482.
9 Bircumshaw, L. L., Philos. Mag., 2 (1926) , 341.
10 Drath, G.; Sauerwald, F., Z. Anorg. Allg. Chem., 162 (1927) , 301.
11 Harvey, D, J., Trans. Metall. Soc. AIME, 221 (1961) , 266.
12 White, D. W. G., Metall. Trans., 2 (1971) , 3067.
13 Greenway, H. T., J. Inst. Met., 74 (1947) , 133.
14 Matuyama, Y., Sci Rap. Tohoku Imp. Univ., 1 (1927) , 16.
15 Lauermann, I.; Sauerwald, F., Z. Metall., 55 (1964) , 605.
16 Lasarew, W.B.; Daschewskij, M.J., DAN, SSSR, 14 (1962) , 822.
17 Hultgren, R.; Orr, R.L.; Anderson, P. D.; Kelley, K. K., Selected Values of Thermodynamic Properties of Metals and Alloys, Univ. of California, Berkeley, 1963, p.893.
18 Eremenko, V.N., The Role of Surface Phenomena in Metallurgy, Consultents Bureau, New York, 1963, p.85.
19#12
No related articles found!