EFFECT OF HEAT OF MIXING ON FORMATION AND STABILITY OF Zr-BASE METALLIC GLASSES
FENG Benzheng; ZHU Yinghua; YANG Rusen (Institute of Precious Metals; Ministry of Metallurgical Industry; Kunming) (Manuscript received 17 April; 1983; revised manuscript 27 October; 1983)
Cite this article: 

FENG Benzheng; ZHU Yinghua; YANG Rusen (Institute of Precious Metals; Ministry of Metallurgical Industry; Kunming) (Manuscript received 17 April; 1983; revised manuscript 27 October; 1983). EFFECT OF HEAT OF MIXING ON FORMATION AND STABILITY OF Zr-BASE METALLIC GLASSES. Acta Metall Sin, 1984, 20(4): 352-357.

Download:  PDF(400KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The glassy alloys, Zr_(1-x)M_x (M=Fe, Co, Ni, Cu and Pd) and Cu_(67.5)Ti_(32.5), were prepared by the melt spinning technique. Their critical tangential speed of the glassy state formation was determined to be 31 m/s by means of changing the tangential speed of rotator. Their structure in a glassy state of all alloy tested has been confirmed by X-ray diffraction analysis. Their thermal behaviour was examined by differential scanning calorimetry (DSC) under different heating rates. An exothermic peak in DSC tracing was presented for glassy alloys Fe_(24)Zr_(76) and Ni_(24)Zr_(76), but two or three peaks for Co_(21)Zr_(79), Pd_(24.5)Zr_(75.5), Cu_(45)Zr_(55) and Cu_(67.5)Ti_(32.5). The activation energies for crystallization of these aUoys were evaluated by the Kissinger's method. Furthermore, the effect of heat of mixing on the formation and stability of these binary glassy alloys has been discussed after calculation used the Miedema's model.
Received:  18 April 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I4/352

1 Takayama, S., J. Mater. Sci., 11 (1976) , 164.
2 Wang, R., Bull. Alloy Phase Diagr., 2 (1981) , №3, 273.
3 Bauhofer, W.; Simon, A., Phys. Rev. Lett., 40 (1978) , 1730.
4 Ohnuma, S.; Shirakawa, W.; Nose, M.; Masumoto, T., IEEE Trans. Magn., MAG-16 (1980) , 1129.
5 Maeland, A. J.; Tanner, L. E.; Libowitz, G. G., J. Less-Common Met., 74 (1980) , 279.
6 Naka, M.; Hashimoto, K.; Masumoto, T.; Okamoto, I., Proc. 4th Int. Conf. on Rapidly Quenched Metals (Sendai 1981) , Eds. Masumoto, T.; Suzuki, K., JIM, Vol. Ⅱ, 1982, p. 1431.
7 Chen, H. S., Acta Metall., 22 (1974) , 1505.
8 Boom, R.; De Boer, F. R.; Miedema, A. R., J. Less-Common Met., 45 (1976) , 237; 46 (1976) , 271.
No related articles found!
No Suggested Reading articles found!