EFFECT OF IMPURITY Zr ON PHYSICAL PROPERTIES OF AMORPHOUS FeZrSiB ALLOYS
ZHANG Zhiying; GUO Huiqun; SHEN Baogen; ZHAN Wenshan (Institute of Physics; Academia Sinica; Beijing) (Manuscript received 27 June; 1983)
Cite this article: 

ZHANG Zhiying; GUO Huiqun; SHEN Baogen; ZHAN Wenshan (Institute of Physics; Academia Sinica; Beijing) (Manuscript received 27 June; 1983). EFFECT OF IMPURITY Zr ON PHYSICAL PROPERTIES OF AMORPHOUS FeZrSiB ALLOYS. Acta Metall Sin, 1984, 20(4): 345-351.

Download:  PDF(474KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Effect of impurity Zr on the magnetic properties, electrical resistivity and thermal stability of amorphous Fe_(82-x)Zr_xSi_5B_(13) (x =0.02, 0.16, 0.87) alloys has been studied. It was observed that while the Zr content in the alloys increases from x=0.02 to 0.87, the crystallization temperature, T_(cr), increases from 755 to 782K at a rate on heating of 10 K/min, and the saturation magnetization, σ(RT), at room temperature also the Curie temperature, Te, decrease 3% and 4.5% respectively. The fluctuation of the exchange interaction of the alloys is increased by the increase of Zr addition. The resistivity minimum was also obtained at low temperature of 15K in the alloy containing Zr=0.87. It seems to attribute this to Kortdo-like effect.
Received:  18 April 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I4/345

1 Hasegawa, R.; O'Handley, R. C., J. Appl. Phys., 50 (1979) , 1551.
2 沈保根;郭慧群;詹文山;陈笃行;章志英;吴宗林;王金玲;潘孝硕,第五届全国磁学会议报告,1983,常熟.
3 Donald, I. W.; Davies, H. A., Rapidly Quenched Metals Ⅲ, 3rd Int. Conf., Univ. of Sussex, Brighton, 1978, Vol. 1, Ed. Cantor, B., London, Mctals Society, 1978, p. 273.
4 沈保根;詹文山,待发表.
5 詹文山,沈保根;郭慧群,低温物理,5(1983) ,91.
6 Luborsky, F. E.; Liebermann, H. H., Appl. Phys. Lett., 33 (1978) , 233.
7 郭慧群;沈保根;陈笃行;潘孝硕,第二届全国非晶态物理讨论会报告,(1980,11,昆明),贵金属2(1981) ,№4,23.
8 Handrich, K., Phys. Status Solidi, 32 (1969) , k55.
9 罗海英;詹文山,待发表.
10 Tsuei, C. C., Amorphous Magnetism Ⅱ, Proc. of the 2nd Int. Symposium on Amorphous Magnetism, Eds. Levy, R. A.; Hasegawa, R., Plenum Press, New York, 1977, p. 181.
11 郭慧群;沈保根;詹文山;潘孝硕,金属学报,19(1983) ,A53.
No related articles found!
No Suggested Reading articles found!