Please wait a minute...
Acta Metall Sin  1984, Vol. 20 Issue (4): 340-344    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF MAGNETIC FIELD-AND TENSIONANNEALING ON MAGNETIC PROPERTIES OF AN Fe_(78)Si_(10)B_(12) METALLIC GLASS
CHEN Duxing (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 25 May; 1983; revised manuscript 20 October; 1983)
Cite this article: 

CHEN Duxing (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 25 May; 1983; revised manuscript 20 October; 1983). EFFECT OF MAGNETIC FIELD-AND TENSIONANNEALING ON MAGNETIC PROPERTIES OF AN Fe_(78)Si_(10)B_(12) METALLIC GLASS. Acta Metall Sin, 1984, 20(4): 340-344.

Download:  PDF(325KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A study was made of the effect of magnetic field-and tension-annealing under temperature below T_c on the permeability of an Fe_(78)Si_(10)B_(12) metallic glass. Two anisotropies induced by magnetization and by strain were observed with K_(um)>0 and K_(us)<0 respectively. The variations of K_(um) and K_(us) with the magnetization and the strain respectively during anneals are reversible basically.
Received:  18 April 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I4/340

1 Luborsky, F. E.; Becker, J. J., IEEE Trans. Magn., MAG-15(1979) , 1939.
2 Narita, K.; Fukunaga, H.; Yamasaki, J.; Hara, K., J. Magn. Magn. Mater., 19 (1980) , 145.
3 Mizoguchi, T.; Hatta, S.; Kato, H.; Arai, H.; Maeda, K.; Akutsu, N., IEEE Trans. Magn., MAG-16 (1980) , 1147.
4 Mitchell, M. A.; Cullen, J. R.; Abbundi, R.; Clark, A.; Savage, H., J. Appl. Phys., 50 (1979) , 1627.
5 O' Handley, R. C., Phys. Rev., B18 (1978) , 930.
No related articles found!
No Suggested Reading articles found!