A STUDY OF EQUILIBRIUM OF Y-S IN MOLTEN Ni~+
WANG Longmei; DU Ting (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 1 August; 1983; revised manuscript 26 November; 1983)
Cite this article: 

WANG Longmei; DU Ting (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 1 August; 1983; revised manuscript 26 November; 1983). A STUDY OF EQUILIBRIUM OF Y-S IN MOLTEN Ni~+. Acta Metall Sin, 1984, 20(4): 286-295.

Download:  PDF(566KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Desulphurization equilibria between Y-S in molten Ni at 1500, 1550 and 1600℃ have been determined and studied thermodynamically. The results are summarized as follows: 1. Temperature dependence of desulphurization constant for the formation of Y-S_(S) as the equilibrium phase in the temperature range of 1500—1600℃ is given by lg K_(YS)=47000/T+20.86 2. Temperature dependences of the first activity interaction parameters between Y and S in liquid Ni are determined to be e_S~Y=350200/T+179 in the temperature range of 1500—1600℃. 3. Temperature dependence of the standard free energy of formation of YS_(S) in liquid Ni is derived to be [Y]_(Ni)+[S]_(Ni)=YS_(S) △G°=-215000+95.53T cal/mol 4. Temperature dependence of the standard free energy of solution of Y in liquid Ni is derived to be Y_(1)=[Y]_(Ni) △G°=126200-79.31T cal/mol 5. Temperature dependences of activity coefficient and selfinteraction coefficient of Y in liquid Ni are derived to be lgγ_Y~0=27584/T-15.151 ∑_Y~Y=-127052/T+69.79 e_Y~Y=-364.8/T+0.2018 6. The minimum content of S in equilibria with Y in liquid Ni in the temperature range of 1500-1600℃ are given ~*[%S]=0.002-0.005 and ~*[%Y]=0.005-0.020. The S content raises with Y when exceed this minimum point.
Received:  18 April 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I4/286

1#12
2 Jacquemot, A.; Gattlier, C., Rapport IRSID, PCM RP, № 63, (1973) .
3 Ejima, A; Suzuki, K-I; Harada, N.; Sanbongi, K., Trans. Iron Steel Inst. Jpn., 17 (1977) , 349.
4 Buzek, Z., Chemical Metallurgy of Iron and Steel, ISI, London, 1973, p. 173.
5 Janke, D.; Fischer, W. A., Arch. Eisenhuettenwes., 49 (1978) , 425.
6 Fischer, W. A.; Ackerman, W., Arch. Eisenuettenwes., 37 (1966) , 43.
7 魏寿昆,钢铁,(1980) ,№ 8,57.
8 王龙妹,杜挺,钢铁研究总院学报,3(1983) ,№1,30.
9 Venal, W. V.; Geiger, G. H., Metall. Trans., 4 (1973) , 2567.
10 Wilson, W. G.; Kay, D. A. R.; Vahed, A.; J. Met., 26 (1974) , № 5, 14.
11 Darken, L. S., Trans. Metall. Soc. AIME, 239 (1967) , 80.
12 Michel Hone; Sergo Houot; Michel Rigand, Can. Metall. Q., 13 (1974) , 619.
13 曲英,炼钢学原理,冶金工业出版社,1980,p.331.
14 冯师颜,误差理论与实验数据处理,冶金工业出版社,1964,p.47.
No related articles found!
No Suggested Reading articles found!