AN EXPRESSION OF STRENGTH OF MARTENSITEFERRITE DUAL PHASE STEELS
SHEN Xianpu; LEI Tingquan (Harbin Institute of Technology) (Manuscript received 18 June; 1983; revised manuscript 22 September; 1983)
Cite this article: 

SHEN Xianpu; LEI Tingquan (Harbin Institute of Technology) (Manuscript received 18 June; 1983; revised manuscript 22 September; 1983). AN EXPRESSION OF STRENGTH OF MARTENSITEFERRITE DUAL PHASE STEELS. Acta Metall Sin, 1984, 20(4): 271-388.

Download:  PDF(1081KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Starting from certain similarities in the structural distribution and the deformation behaviour between the martensite-ferrite dual phase steels and the composite materials reinforced by discontinuous short fibers, a new expression is proposed for the tensile strength of the steels on the basis of the shear lag analysis, i. e. σ_(bDP)=(β/3~(1/2)+0.65)1/Kσ_(bM)V_M+σ_(bF)(1-V_M) where σ_(bDP), σ_(bM) or σ_(bF) is the tensile strength of the steel, the martensite or the ferrite phases respectively, β is the aspect ratio of martensite islands, K is the strength ratio of martensite to ferrite strength, V_M is the volume fraction of martensite and then (1-V_M) is the volume fraction of ferrite. It is in good agreement after quite a few examinations on a variety of dual phase steels with different composition and structure. The load transfer from ferrite to martensite and the utility of strength of martensite have been also discussed.
Received:  18 April 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I4/271

1 田村今男;友田陽;山岡幸男;金谷三郎;小沢正俊;赤尾明;鉄と鋼,59(1973) ,454.
2 Davies, R. G., Metall. Trans., 10 (1979) , 1549.
3 Koo, J. Y.; Young, M. J.; Thomas, G., Metall. Trans., 11A (1980) 852.
4 雷廷权;沈显璞;金属学报,18(1982) ,75.
5 Lei,T.C.(雷廷汉),Liu,G.K.(刘光葵),The Law of Strength of Dual-Phase Steel as Naturally Composite Materials, Paper Presented at ICM-4, Stockholm, Sweden, 1983.
6 Davies, R. G., Metall. Trans., 9A (1978) , 41.
7 友田陽;黑木剛司郎;田村今男;铁と鋼,61(1975) ,107。
8 Araki, K.; Takada, Y.; Nakaoka, K., Trans. Iron Steel Inst. Jpn., 17 (1977) , 710.
9 Tomota, Y.; Kuroki, K.; Mori, T.; Tamura, I., Mater. Sci. Eng., 24 (1976) , 85.
10 Garica, C. I.; Deardo, A. J., Structure and Properties of Daul-Phase Steel, Eds. Kot, R. A.; Morris, J. W., AIME, 1979, p. 40.
11 Szewczyk, A. F.; Garland, J., Metall. Trans., 13A (1982) , 1821.
12 Korzekwa, D. A.; Lawson, R. D.; Matlock, D. K.; Krauss, G., Scr. Metall., 14 (1980) , 1023.
13 Rosen, B. W., Fiber Composite Materials, ASM, Metals Park, Ohio, 1964, Chapter 3.
14 Garland, J., Scr. Metall., 13 (1979) , 967.
15 雷廷权;沈显璞;潘杰,钢铁,18(1983) ,№ 7,46。
16 沈显璞,硕士学位论文,哈尔滨工业大学,1981。
17 Koo, J. Y.; Thomas, G., Formable HSLA and Dual-Phase Steel, Ed. Davenport, A. T., TMSAIME, 1977, p. 40.
18 杨德庄;孙学文;雷廷权,机械工程材料,6(1982) ,№,28.
No related articles found!