EFFECT OF CYCLIC TEMPERATURES ON STRESSRUPTURE LIFE OF A Ni-BASE SUPERALLOY
XIAO Yaotian; TONG Shuqin; XU Zhixian (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 15 December; 1982; revised manuscript 21 April; 1983)
Cite this article: 

XIAO Yaotian; TONG Shuqin; XU Zhixian (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 15 December; 1982; revised manuscript 21 April; 1983). EFFECT OF CYCLIC TEMPERATURES ON STRESSRUPTURE LIFE OF A Ni-BASE SUPERALLOY. Acta Metall Sin, 1984, 20(4): 266-270.

Download:  PDF(805KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The stress-rupture life of a Ni-base superalloy has been evaluated under the cyclic temperatures by using the sinusoidal or the specified program-controlled waveform. It was shown that its stress-rupture life is considerably reduced by the temperature cycle. The extent of reduction is depended on the amplitude of the cycle. The formulation of life prediction for specified program-controlled temperature cycle is proposed. The fracture surface of the superalloy has also been observed by SEM.
Received:  18 April 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I4/266

1 Robinson, E. L., Trans. ASME, 74 (1952) , 777.
2 佟素琴;许志显;肖耀天,理化检验,(1981) ,№.5,15.
3 Miller, J., Symposium on Effect of Cyclic Heating and Stressing on Metals at Elevated Temperature, ASTM STP 165, (1954) , 53.
4 Manson, S. S., Mechanical Behavior of Material at Elevated Temperatures, MaGraw-Hill, New York, 1961, p. 419.
5 Webster, G. A.; Piearcey, B. J., ASM Trans. Q., 59 (1966) , 847.
No related articles found!
No Suggested Reading articles found!