Please wait a minute...
Acta Metall Sin  1984, Vol. 20 Issue (4): 247-382    DOI:
Current Issue | Archive | Adv Search |
INFLUENCE OF Ce ON CRYSTAL MORPHOLOGY OF AUSTENITE AND DENDRITIC SEGREGATION OF Mn IN HIGH-Mn STEEL
HU Hanqi; ZHONG Xueyou; LI Hang (Beijing University of Iron and Steel Technology) (Manuscript received 23 September; 1982; revised manuscript 15 November; 1983)
Cite this article: 

HU Hanqi; ZHONG Xueyou; LI Hang (Beijing University of Iron and Steel Technology) (Manuscript received 23 September; 1982; revised manuscript 15 November; 1983). INFLUENCE OF Ce ON CRYSTAL MORPHOLOGY OF AUSTENITE AND DENDRITIC SEGREGATION OF Mn IN HIGH-Mn STEEL. Acta Metall Sin, 1984, 20(4): 247-382.

Download:  PDF(1412KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Samples of casting high-Mn steel with structure of stable austenitic cells were prepared by strictly controlled directional solidification. With the increasing of the Ce content, the cell structure changes gradually in the front of crystals into dendrites and then into separate crystals, so as to narrow the columnar crystal region. An EPMA was performed quantitatively on the influence of Ce upon the Mn segregation in cellcrystals, columnar and Equiaxial dendrites of high-Mn steel. Considering the solute diffusion in solid state together with the previous works, an expression of Mn distribution in high-Mn steel was approached. After quite a few theoretical analysis on the experimental data, it seems to be indicated that the solute equilibrium partition coefficient, K_0, is the determinant factor of influence on dendritic segregation.
Received:  18 April 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I4/247

1 塗嘉夫;大橋徹郎;広本健,北村修,鉄と鋼,66(1980) ,618.
2 刘树模,稀土元素对钢的枝晶偏析的影响,未发表资料,1979.
3 大橋徹郎;広本健,藤井博務;塗嘉夫;浅野鋼一,铁と鋼,62(1976) ,614.
4 Li Wernbin; Liu Zhengqun; Yang Quoping; Li Chenghsiu; Zhang Bin, Seventh International Conference on Internal Frtction and Ultrasonic Attenuation in Solids, Eds W. Benoit; G. Gremaud, Ecole Polytechnique Federade de Lausanne Instittute de Genie Atomique Ecublens, Lausanne Switzerland, 6-9, July, 1981, Part Ⅰ, C5-463
5 北京钢铁学院物化教研室,钢铁,(1982) ,№ 2,1.
6 钟雪友;胡汉起;刘昌明,高锰钢中Ce的溶液分配系数K_0的测定及Ce对Mn,Si,K_0的影响,北京钢铁学院资料室,1982.
7 Bower, T. F.; Brody, H. D.; Flemings, M. C., Trans. Metall. Soc. AIME, 236 (1966) , 624.
No related articles found!
No Suggested Reading articles found!