Please wait a minute...
Acta Metall Sin  1984, Vol. 20 Issue (3): 261-269    DOI:
Current Issue | Archive | Adv Search |
AN EMPIRICAL CONCEPT ON FORMATION OF BINARY AMORPHOUS ALLOYS BY LIQUID QUENCHING
LIU Zhiyi (Institute of Physics; Academia Sinica; Belling) (Manuscript received 26 April; 1983)
Cite this article: 

LIU Zhiyi (Institute of Physics; Academia Sinica; Belling) (Manuscript received 26 April; 1983). AN EMPIRICAL CONCEPT ON FORMATION OF BINARY AMORPHOUS ALLOYS BY LIQUID QUENCHING. Acta Metall Sin, 1984, 20(3): 261-269.

Download:  PDF(722KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A proposal was made of the increasing tendency of amorphous formation of the binary transition metal alloys caused by the incongruent-and congruent-melting compounds of lower melting temperature on the basis of synthesis of the previous experimental data, including the author's. The effects of crystalline structure, atomic radius difference, electronic structure and electro-negativity difference of eIements were discussed. An empirical approach to the formation of binary amorphous alloys by liquid quenching was summarized. Thus, certain new alloy systems, e.g., Ti-Pd, La-Si, Zr-Ga, Hf-Pd, etc. may be developed.
Received:  18 March 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I3/261

1 Mader, S.; Nowick, A.S.; Widmer, H., Acta Metall, 15(1967) , 203.
2 Fujime, S., Jpn J. Appl. Phys., 6 (1967) , 305.
3 Nowick, A. S.; Mader, S., IBM J. Res. Dev., 9 (1965) , 358.
4 Chen H. S., Acta Metall., 22(1974) , 1505.
5 Alder, B.J., J. Chem. Phys., 40 (1964) , 2724.
6 张邦维,金属学报,17(1981) ,285.
7 Takayama, S., J. Mater. Sci., 11 (1976) , 164.
8 刘志毅,金属学报,20(1984) ,B8.
9 Liu Zhi-yi(刘志毅);Jin Duo(金铎);Jin Zuo-wen(金作文);Ma Ming-rong(马明荣);Zhao Zhong-xian(赵忠贤);Luo Qi-suang(罗启光),Chinese Phys., (1982) ,№2,(Am. Inst. Phys., New York).
10 Donald, I. W.; Davies, H.A., J.Non-Cryst. Solid, 30 (1978) , 77.
11 宁远涛;周新铭,金属学报,17(1981) ,279.
12 Chen, H.S.; Miller, C.E., Rev. Sci. Instrum., 41 (1970) , 1237.
13 Anantharaman, T.R.; Suryanarayana, C., J. Mater. Sci., 6 (1971) , 1111.
14 施天生;郑如龙;陈念贻,金属学报,15(1979) ,94.
15 Chen, H. S.; Jackson, K. A., Metallic Glasses, Papers Presented at Aseminar of the Materials Science Division of the ASM, Sept. 1976, ASM, Metals Park, Ohio, 1978, p. 74.
16 Duwez, P.; Johnson, W. L., J. Less-Common Met., 62 (1978) , 215.
17 Rapp, O.; Lindberg, B.; Chen, H.S.; Rao, K.V., J. Less-Common Met., 62 (1978) , 221.
18 Sommer, F.; Duddek, G.; Predel, B., Z. Metallk., 69 (1978) , 587.
19 刘志毅;王朝果;王守证;王瑜,低温物理,1(1983) ,62.
20 Hansen, M.; Anderko, K., Constitution of Binary Alloys, McGraw-Hill, New York, 1958.
21 Elliott, R. P., Constitution of Binary Alloys, First Suppl., McGraw-Hill, New York, 1965.
22 Hawkins, D.T.; Hultgren, R., Metals Handbook, 8th ed., Vol. 8; Metallographs Structures and Phase Diagrams, ASM, Metals Park, Ohio, 1973.
23 Moffatt's Binary Phase Diagram Handbook, General Electric Company, Schenectady, New York. 1976.
24 1977,
25 鲍林,化学键本质,上海科技出版社,1963,p.422.
26 刘志毅,几种新的非晶态超导合金,全国第四届超导材料学术讨论会论文报告,1982,10. 黄山.y
No related articles found!