CONTROL OF SOLIDIFICATION PROCESS DURING CONTINUOUS CASTING OF STEEL
CAI Kaike (Beijing University of Iron and Steel Technology) LIU Fengrong (Hebei Institute of Mining and Metallurgy) (Manuscript received 18 September; 1982; revised manuscript 14 March; 1983)
Cite this article: 

CAI Kaike (Beijing University of Iron and Steel Technology) LIU Fengrong (Hebei Institute of Mining and Metallurgy) (Manuscript received 18 September; 1982; revised manuscript 14 March; 1983). CONTROL OF SOLIDIFICATION PROCESS DURING CONTINUOUS CASTING OF STEEL. Acta Metall Sin, 1984, 20(3): 252-260.

Download:  PDF(613KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An investigation has been carried out into the "metallurgical criterion" of the slab solidification during continuous casting. The effect of following variables on the metallurgical criterion has been studied by the mathematical model of heat transfer: casting speed, spray water intensity, water distribution in spray zone, superheat in tundish, convection in liquid pool and temperature of spray water. Considering these factors, a nomogram of the productivity related to slab thickness, casting speed, spray water intensity and depth of liquid pool was prepared so as to selecte reasonably the technological parameters and to control scientifically the operation.
Received:  18 March 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I3/252

1 Birat, J. P.; Larrecq, M.; Le Bon, A.; Jeanneau, M.; Poupon, M.; Senaneuch, D., Rev. Metall. (Paris), 79 (1982) , 29.
2 Lair, J. E.; Brimacombc, J. K.; Weinberg, F., Ironmaking Steelmaking, 1 (1974) , № 2, 90.
3 Mizikar, E.A., Trans. Metall. Soc. AIME, 239 (1967) , 1747.
4 Gautier, J. J.; Morillon, Y.; Dumont-fillon, J., J. Iron Steel Inst., 208 (1970) , 1053.
5 Perroy, A., Modéle de Simulation Mathématique de la Coulée Continue, Rapport IRSID, REP. 189, Décembre 1976, Personal Communication.
6 板岡隆;石黑守幸;铁钢凝固,铁钢基础共同会出版,p.199.
7 Fogleman, E. L., J. Met., 26 (1974) , № 10, 31.
No related articles found!
No Suggested Reading articles found!