| THE EFFECTS OF PREAGEING ON SEGREGATION OF P IN A CrMoV TURBINE ROTOR STEEL |
| by QU Zhe (Institute of Metal Research; Academia Sinica; Shenyang); McMAHON C. J.; Jr (University of Pennsylvania; U. S. A.) (Manuscript received 28 December; 1982; revised manuscript 21 September; 1983) |
|
Cite this article:
by QU Zhe (Institute of Metal Research; Academia Sinica; Shenyang); McMAHON C. J.; Jr (University of Pennsylvania; U. S. A.) (Manuscript received 28 December; 1982; revised manuscript 21 September; 1983). THE EFFECTS OF PREAGEING ON SEGREGATION OF P IN A CrMoV TURBINE ROTOR STEEL. Acta Metall Sin, 1984, 20(2): 97-214.
|
|
|
Abstract Temper embrittlement of CrMoV turbine rotor steel with 0.04% P aged at 480℃ after a higher temperature aging for 1000h (preaging) has been compared with that of the conventional heat treated steel with the same composition. The preaging virtually accelerated the rise in transition temperature. This is believed to be conneeted with the depletion of Mo, a scavenger of P, in matrix due to the Mo tithed carbides formation during preaging. Therefore, more P is released and segregated to grain boundaries. Carbide coarsening perhaps contributed to the increment in transition temperature too.
|
|
Received: 18 February 1984
|
1 Gould, G. C., Am. Soc. Test. Mater., Spec. Tech. Publ., №. 407, (1968) , p. 90. 2 Yu, Jin; McMahon, C. J, Jr, Metall. Trans., 11A(1980) , 277. 3 Yu, Jin; McMahon, C. J, Jr, ibid., 291. 4 Qu, Z.; Kuo, K. H., Metall. Trans., 12A(1981) , 1333. 5 Shultz, B. J.; McMahon, C. J., Jr, Am. Soc. Test. Mater., Spec. Tech. Publ., №. 449, (1972) ,p124. 6 Powers A. E., J. Iron Steer Inst., 186(1957) , 323. 7 Low, J. R., Trans. Metall. Soc. AIME, 242(1968) , 14. 8 Greaves, R. H.; Jones, J. A., J. Iron Steel Inst., 111(1925) , 231. 9 #12 10 金子秀夫;西泽泰二;玉置维照;谷藤晓男,日本金属学会志,29(1965) ,166. 11 Kalderon, D., Proc. Inst. Mech. Eng., 186(1972) , 341. 12 Baker, R. G.; Nutting, J., J. Iron Steel, Inst., 192(1959) , 257. 13 Dumoulin, Ph.; Foucalt, M.; Guttmann, M.; Palmier, M.; Wayman, M.; Biscondi, M., Met. Sci., 14(1980) , 1. 14 Qu, Z.; McMahon, C. J., Jr, Metall. Trans., 14A(1983) , 1101. 15 Mclean, D., J. Iron Steel Inst., 174(1953) , 360.j |