| INVESTIGATION ON LCF CRACK GROWTH RATE WITH CONTROLLING DEFLECTION AT HIGH TEMPERATURE |
| by WANG Shuanzhu; CHI Shuyao (Xi'an Aeroengine Factory); GENG Gangqiang (Xi'an Highway Institute) (Manuscript received 3 October; 1982; revised manuscript 5 August; 1983) |
|
Cite this article:
by WANG Shuanzhu; CHI Shuyao (Xi'an Aeroengine Factory); GENG Gangqiang (Xi'an Highway Institute) (Manuscript received 3 October; 1982; revised manuscript 5 August; 1983). INVESTIGATION ON LCF CRACK GROWTH RATE WITH CONTROLLING DEFLECTION AT HIGH TEMPERATURE. Acta Metall Sin, 1984, 20(2): 83-210.
|
|
|
Abstract The low cyclic fatigue (LCF) crack growth rate was measured by means of controlling deflection on a superalloy at 600℃ in open air. The parameter of elastic-plastic fracture mechanics, J-integral was chosen as controlling variable and the relation dα/dN=1.26×10~(-4)(△J)~(1.96) was obtained. It was pointed that how J-integral (△J_t, △J_e, △J_p) varied versus deflection δ within gage length in cyclic loading. The suitableness and limitation were discussed on stress intensity factor △K as controlling variable of a crack growth. Fracture analysis showed that accumulative damage under creep/fatigue interaction made the fracture morphology changed from transgranular striation to intergranular mechanism which characterizes creep fracture.
|
|
Received: 18 February 1984
|
1 Chell, G. G., Colloquium on Fracture, 3rd Fracture & Fatigue, Elasto-Plasticity, Thin-Sheet and Micro-Mechanism Problems, London, 1980, p3-12. 2 Muscati, A., Fracture, 3(1977) , 149. 3 Dowling, N. E., Mechanics of Crack Growth, ASTM, STP, 590,(1976) , p. 82-103. 4 Schwalbe, K. H.; Hellman, D., J. Test. Eval., 9(1981) ,№. 3, 218. 5 Rice, J. R., Progress in Flaw Growth and Fracture Toughness, ASTM, STP, 536, (1973) , p. 231. 6 大路清嗣;小仓敬二:久保司郎,机械の研究,31(1979) ,№.1,33. 7 Dowling, N. E., Crack and Fracture, ASTM, STP 601, (1976) , p. 19-32. 8 Fedderson, C. E., Discussion in Planstrain Crack Toughness Testing of Metallic Materials, ASTM, STP, 410, (1973) , p. 77. 9 陈箎:蔡其巩:王仁智,工程断裂力学,(上册),国防工业出版社,1979,p.368. 10 平修二;田中啓介,小川茂,材料,26(1977) ,№.280,p.93. 11 刘绍伦;谢济洲;未发表资料,1981. 12 Wang Shaunzhu; Yank Cheng; Kang Maokung, Eng. Frac. Mech., 4(1983) . 13 Mowbray, D. E., Crack and Fracture, ASTM, STP, 601, (1976) , p 33. 14 Gabrielli, F.; Pelloux, R. N., Metall. Trans., 13A(1982) , 1083. 15 Chen, I-W; Argon, A. S., Acta Metall., 29(1981) , 1321. |
| No Suggested Reading articles found! |
|
|