Please wait a minute...
Acta Metall Sin  1984, Vol. 20 Issue (2): 112-117    DOI:
Current Issue | Archive | Adv Search |
THERMODYNAMICS OF MARTENSITIC TRANSFORMATION IN LOW ALLOYING MULTICOMPONENT STEELS
by LI Lin (Shandong Institute of Technology); XU Zuyao (T. Y. Hsu) (Shanghai Jiaotong University) (Manuscript received 21 March; 1983)
Cite this article: 

by LI Lin (Shandong Institute of Technology); XU Zuyao (T. Y. Hsu) (Shanghai Jiaotong University) (Manuscript received 21 March; 1983). THERMODYNAMICS OF MARTENSITIC TRANSFORMATION IN LOW ALLOYING MULTICOMPONENT STEELS. Acta Metall Sin, 1984, 20(2): 112-117.

Download:  PDF(419KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An equation for calculating △G intthe martensitic trasformation of the low alloying multicomponent steels has been suggested as: being proved by the mathematic analyses and verified by the practical data of 20CrMnTi steel. The amount of the retained austenite in a hardened steel can be estimated by the equation together with the kinetic formula.
Received:  18 February 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I2/112

1 徐祖耀,金属学报,15(1979) ,329.
2 徐祖耀,马氏体相变与马氏体,科学出版社,1980,p.246.
3 徐祖耀,金属学报,16(1980) ,426.
4 Wada, T.; Wada, H.; Elliott, J. F.; Chipman, J., Metall. Trans., 2(1971) , 2199.
5 Swartz, J. C., Trans. Metall.Soc. AIME, 245(1969) , 1083.
6 Kaufman, L.; Clougherty, E. V.; Weiss, R. J., Acta Metall., 11(1963) , 323.
7 Kaufman, L.; Cohen, M., Trans. AIME, 206(1956) , 1393.
8 徐祖耀,马氏体相变与马氏体,科学出版社,1980,p.260.
9 Davies, R. G.; Magee, C. L., Metall. Trans., 2(1971) . 1939.
10 日本学术振兴会制钢第19委员会,铁纲合金元素,诚文堂新光社,1966,p.670.
11 三本木贡治,大谷,铁钢,47(1961) ,841.
12 Nelson, E. C., Trans. Metall. Soc. AIME, 277(1963) , 189.
13 徐祖耀,金属材料热力学,科学出版社,1981,p.304.
14 热处理手册编委会,热处理手册,第四分册,机械工业出版社,1978,附44.
No related articles found!