THE STRUCTURE RELAXATION SPECTRUM OF METALLIC GLASS
DEN Deguo; YU Jian(Institute of Precious Metals; Ministry of Metallurgical Industry; Kunming) (Manuscript received 24 January; 1983; revised manuscript 30 June; 1983)
Cite this article: 

DEN Deguo; YU Jian(Institute of Precious Metals; Ministry of Metallurgical Industry; Kunming) (Manuscript received 24 January; 1983; revised manuscript 30 June; 1983). THE STRUCTURE RELAXATION SPECTRUM OF METALLIC GLASS. Acta Metall Sin, 1984, 20(1): 87-93.

Download:  PDF(463KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A proposed method for determining the structure relaxation spectra of five metallic glasses of Cu-Zr system has been carried out by measuring the electric resistance at constant heating rate. Three separate peaks of the activation energy with varied frequency factors were shown on the spectrum obtained, The frequency factor influences the shape, range, location and continuity of the peak. The Zr content in the Cu-Zr metallic glasses may affect considerably each own structure relaxation spectrum. Their variaty behaviour has also been discussed.
Received:  18 January 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I1/87

1 Chen, H.S.; Coleman, E., Appl. Phys. Lett., 28 (1976) , 245.
2 Argon, A.S.; Kuo, H.Y., J. Non-Cryst. Solids, 37 (1980) , 241.
3 Vand, V., Proc. Phys. Soc., 55 (1943) , 222.
4 Primak, W., Phys. Rev., 100 (1955) , 1677.
5 Primak, W., J. Appl. Phys., 31 (1960) , 1524.
6 Spaepen, F., Rapidly Quenched Metals Ⅲ, Vol. 2, Proc. of the 3rd Int. Conf. on Rapidly Quenched Metals, hald at Univ. of Sussex, Brighton, U. K., July, 1978, Ed. Cantor, B., The Metals Soc., London, 1978, p. 253.
7 Polk, D.E., Acta Metall., 20 (1972) , 485.
8 Graskell, P.H., Rapidly Quenched Metals Ⅲ, Vol. 2, Pro. of the 3rd Int. Conf. on Rapidly Quenched Metals, hald at Univ. of Sussex, Brighton, U. K., July, 1978, Ed. Cantor, B., The Metals Soc., London. 1978. p. 277.
9 Nanao, S.; Tokumitsu, K.; Matsuzaki, A.; Ino, H.; Nishikawa, S., Structure and Properties of Amorphous Metals Ⅱ, Suppl. to the Science Reports of the Research Institute, Tohoku Univ. Ser. A, Vol. 28, (1980) , 104.
10 Sadoc, J.F.; Lienard, A., ibid. [6] , p. 405.
11 Waseda, Y.; Chen, H.S., ibid. [6] , p. 415.
12 Mizoguchi T.; Kudo, T.; Irisawa, T., ibid. [6] , p. 384.
13 Sakata, M.; Cowlam, N.; Davies, H.A., J. Phys., F, 11 (1981) , L157.
No related articles found!
No Suggested Reading articles found!