EXPERIMENTAL STUDY OF CONDITION FOR BINARY AMORPHOUS ALLOYS FORMATION BY LIQUID QUENCHING
LIU Zhiyi(Institute of Physics; Academia Sinica; Beijing)(Manuscript received 2 August; 1982; revised manuscript 19 November; 1982)
Cite this article: 

LIU Zhiyi(Institute of Physics; Academia Sinica; Beijing)(Manuscript received 2 August; 1982; revised manuscript 19 November; 1982). EXPERIMENTAL STUDY OF CONDITION FOR BINARY AMORPHOUS ALLOYS FORMATION BY LIQUID QUENCHING. Acta Metall Sin, 1984, 20(1): 78-86.

Download:  PDF(809KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An experimental study was carried out on the formation condition of the amorphous state of binary alloys of transition metals. Intermediate phase (incongruent-melting compounds of lower melting temperature and congruent-melting compounds of lower melting temperature)might affect the formation of the amorphous state. A so called "deep eutectic gorge" composition tends more strongly to form an amorphous state. A new amorphous state of binary alloys Hf-Pd has been prepared.A typical structure of amorphous state in binary alloys Sm-Fe was obtained.
Received:  18 January 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I1/78

1 Takayama, S., J. Mater. Sci., 11 (1976) , 164.
2 Gissen, B.C.; Wager, C. N. J., Physics and Chemsitry of Liquid Metals, Ed. Beer, S. Z., Marcel Dekker, New York, 1972, p. 633.
3 Davies, H.A.; Aucote, J.; Hull, J.B., Scr. Metall., 8 (1974) , 1179.
4 Chen, H.S., Acta Metall., 22 (1974) , 1505.
5 Fujime, S., Jpn. J. Appl. Phys., 6 (1976) , 305.
6 Alder, B.J., J. Chem. Phys., 40 (1964) , 2724.
7 Adam, G.; Gibbs, J.H., ibid., 43 (1965) , 139.
8 Donald, L W.; Davies, H.A., J. Non-Cryst. Solids, 30 (1978) , 77.
9 Cohen, H, M.; Turnbull, D., Nature, 189 (1961) , 131.
10 Mader, S.; Nowick, A.S.; Widmer, H., Acta Metall., 15 (1967) , 203.
11 施天生;郑如龙;陈念贻,金属学报,15(1979) ,94.
12 宁远涛;周新铭,金属学报,17(1981) ,278.
13 张邦维,金属学报,17(1981) ,285.
14 Hansen, M.; Anderko, K., Constitution of Binary Alloys, McGraw-Hill, New York, 1958, p. 28, 212, 592.
15 Graebner, J.E.; Golding, B.; Schultz, R.J.; Hsu, F. S. L.; Chen, H. S., Phys. Rev. Lett., 39 (1977) , 1480.
16 Liu Zhi-yi (刘志毅); Jin Duo (金铎); Jin Zup-wen (金作文; Ma Ming-rong (马明荣); Zhao Zhong-xian (赵忠贤); Luo Qi-guang (罗启光), Chin. Phys., 2 (1982) , 486.
17 Liu Zhi-yi (刘志毅); Wang Chao-guo (王朝果); Cheng Peng-zhu (程鹏煮); Yang Da-yu (杨大宇); Ma Xiao-hua (马小华); Luo Qi-quang (罗启光), Chin. Phys., 2 (1982) , 489.
18 #12
19 Moffatt's Binary Phase Digram Handbook, General Electric Co., 1976.
20 刘志毅;王守证,低温物理,3(1981) ,235.
21 刘志毅;毕文;刘振兴,低温物理,2(1980) ,144
No related articles found!
No Suggested Reading articles found!