Please wait a minute...
Acta Metall Sin  1984, Vol. 20 Issue (1): 54-61    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF Cu ON PRECIPITATION AND STRUCTURAL PARAMETERS OF Al-Zn-Mg ALLOY
LIN Zhaoqi; ZHU Jiliang; SUN Guijing; YANG Shengkun (Northeast Institute of Technology; Shenyang) (Manuscript received 4 March; 1983; revised manuscript 12 July; 1983)
Cite this article: 

LIN Zhaoqi; ZHU Jiliang; SUN Guijing; YANG Shengkun (Northeast Institute of Technology; Shenyang) (Manuscript received 4 March; 1983; revised manuscript 12 July; 1983). EFFECT OF Cu ON PRECIPITATION AND STRUCTURAL PARAMETERS OF Al-Zn-Mg ALLOY. Acta Metall Sin, 1984, 20(1): 54-61.

Download:  PDF(1160KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of a trace of Cu, about 0.19 wt-%, on the precipitation, the critical nucleation temperature, T_c~′, as well as the microstructural parameters of a commercial purity Al-S.0Zn-1.75Mg alloy has been studied by means of hardness test, optical microscopy and TEM. It was resulted that Cu, in contrast to Cr, is an element by which its homogeneous precipitation is promoted, the T_c~′ is raised from 150—160℃ to 170—180℃ and the hardness is increased, but the grain size is not yet refined and the recrystallization is not yet inhibited. Under the experimental condition of 120—200℃ aging, the grain boundary precipitation, the matrix precipitation and the precipitation-free zone of the Cu-contained alloy are minor to that of Cu-free one. All of these alteration may be monotoneous with elongation of aging time and elevation of aging temperature. Thus, it was proposed that the effect of Cu added on the precipitation and the structural parameters may he explained by a nucleation model which a complex cluster of the vacancy-tetrahedron combined with the segregated solute atoms, such as Zn, Mg and Cu, acts as a nucleus of GP zone.
Received:  18 January 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I1/54

1 Polmear, I.J., Met. Prog., 81 (1962) , 82.
2 Kent, K.G., Weld. Met. Fabr., 35 (1967) , 280.
3 Busby, J.; Cleave, J. F.; Cudd, R.L., J. Inst. Met., 99 (1971) , 41.
4 Truscott, J. M.; Carter, V.E.; Campbell, H.S., ibid., 99 (1971) , 57.
5 林肇琦;孙贵经;许海峰,东北工学院学报,27(1981) ,23.
6 Polmear, I.J.; Scott-Young, P., J. Inst. Met., 87 (1958/59) , 65.
7 Polmear, I.J., ibid., 89 (1960/61) , 51.
8 Smith, W.F.; Grant, N.J., Metall. Trans., 2 (1971) , 1333.
9 馬場義雄,日本金属学会誌 31(1967) ,507.
10 馬場義雄,ibid.,31(1967) ,513.
11 林肇琦;封冰;孙贵经;杨胜坤,金属学报,19(1983) ,A 197.
12 Embury, J.D.; Nicholson, R.B., Acta Metall., 13 (1965) , 403.
13 Lorimer, G.W.; Nicholson, R.B., ibid., 14 (1966) , 1009.
14 Guy、A、G.;Hren,J.J.,物理冶金学原理,徐纪南主译,机械工业出版社,1981,p.276.
15 Noble, B., Acta Metall., 16 (1968) , 393.
16 Smallman,R.E.,现代物理冶金学,张人佶译,冶金工业出版社,1980,p.210.
17 杨胜坤;孙贵经;林肇琦,待发表.
18 Adler, P.; DeIasi, R, ; Geschwind, G., Grumman Research Department Memorandum RM52, November 1971.
19 Thomas, G.; Nutting, J., J. Inst. Met., 88 (1959/60) , 81.f
No related articles found!
No Suggested Reading articles found!