EFFECT OF ESR ON CONSTITUTION NEARBY GRAIN BOUNDARY IN A Co-BASE SUPERALLOY
DAI Tongfu; WANG Shuhe; SHI Changxu (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 2 August; 1982; revised manuscript 25 January;1983)
Cite this article: 

DAI Tongfu; WANG Shuhe; SHI Changxu (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 2 August; 1982; revised manuscript 25 January;1983). EFFECT OF ESR ON CONSTITUTION NEARBY GRAIN BOUNDARY IN A Co-BASE SUPERALLOY. Acta Metall Sin, 1984, 20(1): 47-148.

Download:  PDF(2013KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of the electroslag remelting (ESR) on the constitution nearby the grain boundary in a Co-base superalloy, Co-22Ni-22Cr-14W, during 760℃ aging has been investigated by Auger electron spectrum. Results show that the segregation of alloying elements toward the grain boundary is of various extents by the influence of ESR: the segregation of La may be decreased, and of P and S more markedly; That of Cr may also be decreased, but not obviously yet of W. At the beginning of aging, the segregation of C toward the vicinity of the grain boundary may be obstructed by ESR, and with the prolongation of aging time, it might be accelerated.
Received:  18 January 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I1/47

1 Bhat, G, K.; Tobias, J.B.; Kennard, R.L., Second International Symposium on Electroslag Remelting Technology, Symp. Proc. Part one, Ed. Bhat, G.K., Pennsylvania, 1969.
2 #12
3 Heslop, J.; Knott, A.R., Met. Mater., 5 (1971) , No. 2, 59.
4 #12
5 Mclean, D., Grain Boundaries in Metals, Oxford, 1957, pp. 116--149.
6 Handbook of Auger Electron Spectroscopy, 2nd, Ed. Palmberg, P.W., Phys. Electr. Ind. Inc., Minnesota, 1976, pp. 5-10.
7 Aerospace Structural Metals Handbook, Eds. Wolf. J.; Brown, Jr., W.F., Belfour Stulen Inc., Watertown, Mass., 1975, Code 4310.
8 #12
9 Walsh, J. M; Anderson, N.P., Superalloys-Metallurgy and Manufacture, Proc. of the Ⅲ Int. Symp., Eds. Kear, B.H.; Muzyka, D.R., et al., Baton Rouge Clator's Publ., 1976, pp. 127-136
10 Yamagnchi, S., Met. Technol, 6 (1979) , 170.
11 曲哲,郭可信,金图学报,16(1980) ,371./
No related articles found!
No Suggested Reading articles found!