PROPOSAL FOR A DIFFERENTIAL EQUATION OF TENSION IN TANDEM ROLLING
WANG Guodong (Northeast Institute of Technology; Shenyang)(Manuscript received 23 April; 1983)
Cite this article: 

WANG Guodong (Northeast Institute of Technology; Shenyang)(Manuscript received 23 April; 1983). PROPOSAL FOR A DIFFERENTIAL EQUATION OF TENSION IN TANDEM ROLLING. Acta Metall Sin, 1984, 20(1): 117-122.

Download:  PDF(378KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A differential equation of tension in tandem rolling was proposed as: dσ_(fi)/dt=E/(h_i integral from n=0 to L (dx)/(h(x)))(v_(i+1)~′-v_i) It seems to be satisfied for those rolling processes of both uniform and variant strip section. The equation may be simplified to one for uniform strip section if it operated through the stands uniformly. Based on the derivation and discussion of the equation an approach to applying the conventional tension differential equation for the computation of the rolling process of variant gage without introducing any error would be incorrect.
Received:  18 January 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I1/117

1 张树堂;刘玉荣,金属学报,17(1981) ,206.
2 张进之,金属学报,18(1982) ,755.
No related articles found!
No Suggested Reading articles found!