STRUCTURE MICROANALYSIS OF INTERFACE BETWEEN Cu-Ti ALLOY AND DIAMOND (OR GRAPHITE)
GAO Qiaojun (Department of Physics; Peking University)
Cite this article: 

GAO Qiaojun (Department of Physics; Peking University). STRUCTURE MICROANALYSIS OF INTERFACE BETWEEN Cu-Ti ALLOY AND DIAMOND (OR GRAPHITE). Acta Metall Sin, 1983, 19(6): 92-99.

Download:  PDF(2188KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The structure of micro-region along the interfacial section between Cu-Ti alloy and graphite (or diamond) has been analyzed by using SEM-EDS and SEMWDS as well as in-depth metallography and X-ray diffraction. It was revealed that the wetting and bonding behaviour on diamond surface by Cu-Ti melt is realized through the stable TiC film which is produced by interaction between Ti atoms of Cu-Ti alloy and C atoms of graphite (or diamond) surface at elevated temperatures.
Received:  18 June 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I6/92

1 Mortimer, D. A.; Nicholas, M., J. Mater. Sci., 5 (1970) , 149.
2 Mortimer, D. A.; Nicholas, M., ibid., 8 (1973) , 640.
3 Scott, P. M.; Nicholas, M., ibid., 10 (1975) , 1833.
4 Standing, R.; Nicholas, M., ibid., 13 (1978) , 1509.
5 Kizikov, E. D., Met. Sci. Heat Treat., 17 (1975) , 61.
6 林增栋;徐乍英,未公开发表资料,1979.
7 林增栋;未公开发表资料.
8 林增栋;徐乍英;杨伟光,未公开发表资料,1981.
9 Joukainen, A.; Grant, N. J.; Floe, C. F., Trans. AIME,, 194 (1952) , 766.
No related articles found!
No Suggested Reading articles found!