Acta Metall Sin  1983, Vol. 19 Issue (6): 86-91    DOI:
Current Issue | Archive | Adv Search |
SPATIAL ORIENTATION DISTRIBUTION OF CRYSTALLITES IN COLD-ROLLED Al-KILLED STEEL SHEET DURING RECRYSTALLIZATION ANNEALING
HUANG Qingzhu; KONG Bingyu; ZHU Congxun (Research Institute of Wuhan Iron and Steel Company)
Cite this article: 

HUANG Qingzhu; KONG Bingyu; ZHU Congxun (Research Institute of Wuhan Iron and Steel Company). SPATIAL ORIENTATION DISTRIBUTION OF CRYSTALLITES IN COLD-ROLLED Al-KILLED STEEL SHEET DURING RECRYSTALLIZATION ANNEALING. Acta Metall Sin, 1983, 19(6): 86-91.

Download:  PDF(538KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The change of texture during recrystallization annealing in low carbon Alkilled steel sheet containing 0.13% Cu has been studied by function of crystal orientation distribution. It is shown that the cold-rolled texture is composed of one component of the <111> fibre texture with fibre axis parallel to the plane normal and another component of {001} <110>. The <110> partial fibre texture with fibre axis parallel to the rolling direction is formed by the diffusion of the two components. During the recrystallization, <111> fibre texture becomes prevailing and {001} <110> component diminishes while the <110> partial fibre texture contracts gradually, therefore, the <110> partial fibre texture is not an independent one.
Received:  18 June 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I6/86

1 Michalak, J. T.; Schoone, R. D., Trans. Metall. Soc. AIME, 242 (1968) , 1149.
2 Stickels. C. A.. Trans. Metall. Soc. AIME. 236 (1966) . 1295.
3 高橋政司;岡本篤樹,铁鋼,61 (1975) ,2246.
4 花井諭;竹本長靖;山水弥一郎,佐直康則,铁鋼,57(1971) ,386.
5 周永忻;黄清珠;陈乾惕;邓定庆;蒲绍康,金属学报,14 (1978) ,292.
6 阿部秀夫;鈴木竹四;户川史江,铁鋼,60 (1974) ,217.
7 Bunge, H. J.; Robert, W. T., J. Appl. Cryst., 2 (1969) , 116.
8 Heckler, A. J.; Granzow, W. G., Metall. Trans., 1 (1970) , 2089.
9 梁志德;徐家祯;王福,金属学报,16 (1980) ,276.
10 Roe, R. J., J. Appl. Phys., 36 (1965) , 2024.
11 Bunge, H. J. Z. Metallk., 56 (1965) , 872.
12 Rickett, R.L.; Leslie, W, C., Trans. ASM, 51 (1959) , 310.T
No related articles found!
No Suggested Reading articles found!