AN INVESTIGATION ON LIQUIDUS OF Al-RICH CORNER OF Al-Mg-La SYSTEM
ZHENG Chaogui; XING Ya; QIAN Jiuxin; YE Yupu (Department of Chemistry; peking University)
Cite this article: 

ZHENG Chaogui; XING Ya; QIAN Jiuxin; YE Yupu (Department of Chemistry; peking University). AN INVESTIGATION ON LIQUIDUS OF Al-RICH CORNER OF Al-Mg-La SYSTEM. Acta Metall Sin, 1983, 19(6): 61-66.

Download:  PDF(495KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The liquidus of the Al-rich corner in the phase diagram of Al-Mg-La system has been investigated by means of thermal, metallographic and X-ray diffraction techniques. The composition of all samples was determined accurately by chemical analysis. It was found that the pseudo-ternary system Al-Mg_5Al_8-LaAl_4 is of the ternary eutectic type. There are three surfaces corresponding to the primary crystallization of a-Al, Mg_5Al_8 and LaAl_4 respectively, and three univariant lines related to the secondary crystallization. The temperature of the ternary eutectic, composed of 11.3 wt-% La, 62.9 wt-% Al and 25.8 wt-% Mg, was determined to be 445℃.
Received:  18 June 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I6/61

1 Weibke, F.: Schmidt, W., Z. Elektrochem., 46 (1940) , 357.
2 Mondolfo, L. F., Aluminum Alloys: Structure and properties, Butterworth, London, 1976, p. 307, 311.
3 Hansen, M.; Anderko, K., Constitution of Binary Alloys, McGraw-Hill, New York, 1958, p. 102, 105.
4 #12
No related articles found!
No Suggested Reading articles found!