EFFECT OF STRUCTURE AND TEXTURE ON COLD WORKABILITY OF 3%-AND 4%Si-Fe ALLOYS
LU Qichun; ZHANG Wenrun; SHUAI Renjie; LI Junyi (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing)
Cite this article: 

LU Qichun; ZHANG Wenrun; SHUAI Renjie; LI Junyi (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). EFFECT OF STRUCTURE AND TEXTURE ON COLD WORKABILITY OF 3%-AND 4%Si-Fe ALLOYS. Acta Metall Sin, 1983, 19(6): 36-44.

Download:  PDF(2810KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of the hot-rolling microstructure and texture on the cold workability of 3%-and 4%Si-Fe alloys has been studied by the cold-rolling and bending tests. The plasticity of the hot-rolled plate would be better by making the grains fine and improving the homogeneity in the hot-rolled structure. The cold-rolling test of the single crystal with specific orientation shows that it is benefited in the ductility of cold-rolling by increasing {112} <110> and {111} <112> among the main hotrolled texture.
Received:  18 June 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I6/36

1 Arai, K.I. Tsuya, N.; Ohmori, K.; Shimanaka, H.; Miyazaki, T., J. Magn Magn Mater, 15-18 (1980) , 1425.
2 Narita, K.; Teshima, N.; Agano, T.; Funahashi, H., IEEE Trans. Magn., MAG-16 (1980) , 517.
3 Fiedler, H.C., J. Iron Steer Inst., 205 (1967) , 158.
4 Burr, D.J.; Butt, R.J.; Wakeman, D.W., J. Iron Steer Inst., 203 (1965) , 500.
5 #12
6 #12
7 Clark, C.A.; Mason, J.J., Patent Specification, №982 101, 1965. (England).
8 Clark, C.A.; Mason, J.J.; Mee, P.B., Proc. IEE, 113 (1966) , №2, 345.
9 吕其春;张文润;李军;李俊义,冶金因素对高硅硅钢冷加工性能的影响,待发表.
10 Lu Qichun; Shuai Renjie; Zhou Xiuyuan, Proc. of the 6th Int. Conf. on Textures of Materials, Vol. 2, 1981, Tokyo, Ed. Nagashima, S.I., Publ. Iron and Steel Inst. Jpn, p.958-966.
No related articles found!
No Suggested Reading articles found!