Please wait a minute...
Acta Metall Sin  1983, Vol. 19 Issue (5): 81-156    DOI:
Current Issue | Archive | Adv Search |
STRESS CORROSION CRACKING OF AUSTENITIC STAINLESS STEEL UNDER COMPRESSIVE STRESS
YAO Jing; CHU Wuyang; XIAO Jimei (Beijing University of Iron and steel Technology)
Cite this article: 

YAO Jing; CHU Wuyang; XIAO Jimei (Beijing University of Iron and steel Technology). STRESS CORROSION CRACKING OF AUSTENITIC STAINLESS STEEL UNDER COMPRESSIVE STRESS. Acta Metall Sin, 1983, 19(5): 81-156.

Download:  PDF(2803KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Experiments were conducted in the stress corrosion cracking (SCC) of the austenitic stainless steel in boiling 42% MgCl_2 solution under compressive stress using three different types of specimens with surface residual compressive stress; of U-bend or of notched modified WOL. The SCC was observed on them after 110, 73—100 or 262—324 h respectively. Their fracture surface are charaterized by the stratified rock structure and the striation-like pattern of quasi-cleavage rather than the river marks or the fan pattern under the tensile stress. Almost one order of magnitude of the incubation period of SCC under the compressive stress is prolonged beyond that under tension. Because the cracking propagates very slowly and spreads hardly to distinguish, the SCC under compressive stress does not be revealed, if it is under tensile stress simultaneously. The behaviour of hydrogen in SCC of such system has been also discussed.
Received:  18 May 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I5/81

1 Brown, B. F., Stress Corrosion Creacking of Metals, ASTM-STP 518, 1976, p. 82.
2 褚武扬;肖纪美;李世琼,金属学报,16 (1980) ,179;17 (1981) ,10;18 (1982) ,47.
3 Chu, W. Y.(褚武扬);Hsiao, C. M.(肖纪美);Li, S. Q.(李世琼),Corrosion,36(1980) ,475;37 (1981) ,320;514.
4 褚武扬;肖纪美;王枨;朱淑彦,金属学报,18 (1982) ,515.
5 Chu, W. Y.(褚武扬);Hsiao, C. M.(肖纪美);Ju, S. Y.(朱淑彦);Wang, C.(王枨),Corrosion, 38 (1982) ,446.
6 Hoar, T. P., Corrosion, 19 (1963) , 331t.
7 Scheil, M. A., Symposium on Stress Corrosion Cracking, AIME, 1945, p. 425.
8 褚武扬编著,断裂力学基础,科学出版社,1979,p.163.
9 Takano, M.; Takaku, H., Corrosion, 37 (1981) , 142.
10 Yang, L, Physical Metallurgy of Stress Corrosion Fracture, Ed. Rhodin, T. N., Interscience, New York, 1959, p. 29.
11 姚京;褚武扬;肖纪美,不锈钢的氢致滞后开裂,待发表.
12 Rhodes, P. R., Corrosion 25 (1969) , 462.