Please wait a minute...
Acta Metall Sin  1983, Vol. 19 Issue (5): 69-80    DOI:
Current Issue | Archive | Adv Search |
A NOTE ON FRACTURE MECHANICS PARAMETERS OF DISK INCLUSIONS
JIANG Shengrui; ZHANG Hongtu (Lanzhou University)
Cite this article: 

JIANG Shengrui; ZHANG Hongtu (Lanzhou University). A NOTE ON FRACTURE MECHANICS PARAMETERS OF DISK INCLUSIONS. Acta Metall Sin, 1983, 19(5): 69-80.

Download:  PDF(733KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The expression of the elastic field round the outside of the disk inclusion has been deduced analytically by the method of the harmonic and biharmonic potentials. The formulation of the stress intensity factors of the disk inclusions in terms of its eign-strains is resulted. The aspects of the results obtsined as well as its availability have also been discussed.
Received:  18 May 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I5/69

1 Bilby, B.A.; Eshelby, J.D., Fracture, Vol.1: Microscopic and Macroscopic Fundamentals, Ed. Liebowitz, H., Academic Press, 1968, p.99.
2 张宏图,折晓黎,物理学报,30(1981) ,761.
3 折晓黎,张宏图,ibid.,32 (1983) ,182.
4 徐祖耀,马氏体相变和马氏体,科学出版社,1980,p.103.
5 Esheby, J.D., Proc. R. Soc., A241 (1957) , 376.
6 Esheby, J. D., ibid., A252 (1959) , 561.
7 Esheby, J.D., Progress in Solid Mechanics, Vol. Ⅱ, Eds. Snedden, I.N., Hill, R., North-Holland, 1961, p.87.
8 村外志夫;森勉,転位介在物,培风馆,1976,p.23.
9 Kroener, E., Z. Phys., 151. (1958) , 504.
10 Macmillan, W. D., The Theory of the Potential, Dover Publ., New York, 1958, p.62.
11 北京钢铁研究院金属物理室,工程断裂力学,上册,国防工业出版社,1977,p.53,54.
12 Tada, H.; Paris P.C.; Irwin, G., The Stress Analysis of Cracks Handbook, Hellerlown, Pennsylvania, 1973, p.24. 1, 24. 7.
13 Esheby, J.D., Solid State Physics, Vol.3, Eds. Seilz, F.; Turnbull, D., Academic Press, New York, 1956, p.79.
14 Hull, D., Acta Metall., 9 (1961) , 191.y
No related articles found!