EFFECTS OF AS-CAST CRYSTALLINE STRUCTURE AND Cu SEGREGATION ON COERCIVITY OF Sm (Co, Cu, Fe, Mn)_(7.8) PERMANENT MAGNET
JIANG Jingkai; XIAO Lianfang; WANG Jiahai (Baotou Research Institute of Metallurgy)
Cite this article: 

JIANG Jingkai; XIAO Lianfang; WANG Jiahai (Baotou Research Institute of Metallurgy). EFFECTS OF AS-CAST CRYSTALLINE STRUCTURE AND Cu SEGREGATION ON COERCIVITY OF Sm (Co, Cu, Fe, Mn)_(7.8) PERMANENT MAGNET. Acta Metall Sin, 1983, 19(5): 65-154.

Download:  PDF(1620KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Effects of the as-cast crystaline structure and segregation in Cu on the coercivity of Sm(Co, Cu, Fe, Mn)_(7.8) permanent magnets have been investigated. Experimental results showed that the crystalline structure of the ingot is different with different cooling rates. In the equi-axed grain structure, the inner of the grain is deficient in Cu; free Cu concentrates on the grain boundaries, where an amount of high temperature phase of hexagonal structure of Sm_2Co_(17-x)T_x is preserved, resulting in a decrease in the coercivity. In the fine-columnar grain structure, no serious segregation in composition has been observed. Magnets after sintering and solution treatment exhibit the cellular microstructure; precipitated Cu and SmCo_(5-x)T_x phase rich in Cu disperse on the cell-wall. They probably play, in the course of magnetization reversal, the role of pinning the domain wall, hence, giving high coercivity.
Received:  18 May 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I5/65

1 Livingston, J.P.; Martin, D.L., J. Appl. Phys., 48 (1977) , 1350.
2 Nagel, H.; Menth, A., IEEE Trans. Math., MAG-12 (1976) , 1961.
3 Sun Daku; Liu Yujin, Proc. 5th Int. Workshop on Rare Earth-Cobalt Permanent Magnets and Their Application, Roanoke, Virginia. (USA), June, 1981, p. 525.
4 Yoneyama, T.; Fukuno, A.; Ojima, T., Proc. 4th Int. Workshop on Rare Earth-Cobalt Permanent Magnets and Their Application, Hakome National Park, Jpn., May, 1979, p.407.
5 Shimoda, T.; Okonogi, I; Teraishi, K., Proc, 5th Int. Workshop on Rare Earth-Cobalt Permanent Magnets and Their Application, Roanoke, Virginia(USA), June, 1981, p.595.
6 Mishra, R. K.; Thomas, G., Proc. 4th Int. Workshop on Rare Earth-Cobalt Permanent Magnets and Their Application, Hakone National Park, Jpn., May. 1979, p.301.
7 杨应昌;何文旺;林勤,待发表.
8 金子秀夫,日本金属学会会报,2 (1976) ,109.
No related articles found!
No Suggested Reading articles found!