ANNEALING AND TEMPERATURE DEPENDENCE OF MAGNETOSTRICTION IN NEARLY ZERO-MAGNETOSTRICTIVE METALLIC GLASSES
CHEN Duxing (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing)
Cite this article: 

CHEN Duxing (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). ANNEALING AND TEMPERATURE DEPENDENCE OF MAGNETOSTRICTION IN NEARLY ZERO-MAGNETOSTRICTIVE METALLIC GLASSES. Acta Metall Sin, 1983, 19(5): 58-64.

Download:  PDF(536KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The variations of the magnetostriction in certain nearly zero-magnetostrictive metallic glasses with annealing and temperature were studied. It was found that, with the increasing of annealing temperature, the magnetostriction goes up then down and contains some reversible component; with the increasing of measuring temperature, it goes up to a small plus value and then down to zero at Curie temperature. The experimental phenomena were interpreted roughly in the light of concepts of structure relaxation, initial crystallization and the single-ion and twoion models about magnetostriction.
Received:  18 May 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I5/58

1 Sherwood, R.C.; Gyorgy, E. M.; Chen, H.S.; Ferris, S.D.; Norman, G,; Leamy, H.J., AIP Conf. Proc., (1975) , № 24. , 745.
2 Kikuchi, M.; Fujimori, H.; Obi, Y.; Masumoto, T., Jpn. J. Appl. Phys., 14 (1975) , 1077.
3 Gyorgy, E. M.; Leamy, H. J.; Sherwood, R. C.; Chen, H.S., AIP Conf. Proc., (1976) , №29, 198.
4 O'Handley, R.C.; Mendelsohn, L.I.; Nesbitt, E.A., IEEE Trans. Magn., MAG-12 (1976) , 942.
5 Kohmoto, O.; Yamaguchi, N.; Ohya, K.; Fujishima, H.; Ojima, T., IEEE Trans. Magn., MAG-14 (1978) , 949.
6 Kohmoto, O.; Ohya, K.; Yamaguchi, N.; Fujishima, H.; Ojima, T., J. Appl. Phys., 50 (1979) , 5054.
7 Ohnuma, S.; Masumoto, T., J. Appl. Phys., 50(1979) , 7597.
8 Hilzinger, H.R.; Hillmann, H.; Mager, A,, Phys. Status Solidi, A55 (1979) , 763.
9 Hilzinger, H. R.; Kunz, W., J. Magn. Magn. Mater., 15-18 (1980) , Part Ⅲ, 1357.
10 陈笃行,加张力测量非晶软磁带样λ_s的冲击法,待发表.
11 O'Handley, R.C., Phys. Rev., B18 (1978) , 930.
12 O'Handley, R.C.; Sullivan, M.O.,J. Appl. Phys., 52 (1981) , 1841.
13 Egami, T., Mater. Res. Bull., 13 (1978) , 557.
14 Egami, T., J. Mater. Sci., 13 (1978) , 2587.
15 Bozorth, R.M., Ferromagnetism, D.Van Nostrand-Co, New York, 1956, p.664.
No related articles found!
No Suggested Reading articles found!