EFFECT OF ROTATIONAL FIELD ANNEALING ON MAGNETIC ANISOTROPY OF Fe_5Co_(73)Si_(10)B_(12) AMORPHOUS ALLOY
GUAN Kehong; SUN Tinglie; LI Donghui (Northeast Institute of Technology; Shenyang)
Cite this article: 

GUAN Kehong; SUN Tinglie; LI Donghui (Northeast Institute of Technology; Shenyang). EFFECT OF ROTATIONAL FIELD ANNEALING ON MAGNETIC ANISOTROPY OF Fe_5Co_(73)Si_(10)B_(12) AMORPHOUS ALLOY. Acta Metall Sin, 1983, 19(5): 53-57.

Download:  PDF(366KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Ribbon specimens were prepared from Fe_5Co_(73)Si_(10)B_(12) amorphous alloy and quenched, annealed or rotational field annealed separately. According to the variation on the magnetization and the magnetostriction figures with different annealed states of them, the magnetic anisotropy induced by the spontaneous magnetization field may be released by the rotational field annealing for such ahoy of which the Curie point is lower than the crystallizing temperature. Th ereason why the amorphous ahoy as-quenched is magnetic anisotropy has been analyzed and discussed.
Received:  18 May 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I5/53

1 Hiroaki Morita; Hiroyasu Fujimoro; Yoshihisa Obi, Jpn. J. Appl. Phys., 18 (1979) , 683.
2 Hiroyasu Fujimori; Tsuyoshi Masumoto, Suppement to Sci Rep., The Research Institute for Iron, Steel and Other Metals, Tohoku University, Sendai, Jpn., 1978, p. 181.
3 Hiroyasu Fujimori, Magnetic Anisotropy, Ed. Luborsky (unpublished).
4 Tsunashima, S.; Maehata, Y.; Uchiyama, S., IEEE Trans. Magn., MAG-17 (1981) , 3073
No related articles found!
No Suggested Reading articles found!