TRANSFORMATION OF Ni-Ti SHAPE MEMORY ALLOY
CHEN Lijun; ZHOU Qinyou; HONG Weiqing (Shanghai Institute of Iron and Steel Research)
Cite this article: 

CHEN Lijun; ZHOU Qinyou; HONG Weiqing (Shanghai Institute of Iron and Steel Research). TRANSFORMATION OF Ni-Ti SHAPE MEMORY ALLOY. Acta Metall Sin, 1983, 19(5): 21-26.

Download:  PDF(980KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The transformation of the equal atom Ni-Ti shape menory alloy has been studied at 150℃ by means of X-ray diffraction, internal friction, electric resistance and TEM. It was shown that two kinds of phase transformation, namely, of the martensite and the R-phase in the alloy are done between 40-50℃. The structure of martensite and of R-phase is distorted monoclinic B_(19) and B_2 respectively. The Rphase does not reveal a pre-transformation and remains relative stable till -185℃. Thus, the phase transformation in an equal atom Ni-Ti alloy takes place as:β(?)β+R+M(B_(19))(?)R+M(B_(19)).
Received:  18 May 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I5/21

1 Wang, F. E.; Buchler, W.J.; Pickart, S.J., J Appl. Phys., 36 (1965) , 3232.
2 De Lange, R.G.; Zijderveld, J.A., J. Appl. Phys., 39 (1968) , 2195.
3 Perkins, Jeff, Metall. Trans., 4 (1973) , 2714.
4 Wang, F.E.; Pickart, S. J.; Alperin, H. A., J Appl. Phys., 43 (1972) , 97.
5 Ling, H.C.; Kaplow, R., Metall. Trans., 11A (1980) , 77.
6 Chandra, K.; Purdy, G. R., J. Appl. Phys., 39 (1968) , 2176.
7 Sandrock, G.D.; Perkins, A.J.; Hehemann, R. F., Metall. Trans., 2 (1971) , 2769.
8 Khachin, V. H.; Paskal, Yu, I.; Gunter, V.E.; Monasevich, A.A.; Sivokha, V.P., Phys. Met. Metallogr. 46 (1978) , №3, 49.
9 沈善初;王惠芝,稀有金属结构与性能测试文集,宝鸡有色金属研究所,1981,p.46.
10 Knowles, K.M.; Smith, D.A., Acta Metall., 29 (1981) , 101.
11 冯端;王业宁,丘第荣,金属物理,下册,科学出版社,1975,p.609.
No related articles found!
No Suggested Reading articles found!